MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 3499-3 X 113393 A Liquid Crystal Polymer (LCP), Glass Fiber - LDS Platable
Categories: Polymer; Thermoplastic; Liquid Crystal Polymer (LCP)

Material Notes: Dielectric Constant K: 4.18 at 1 GHz, 4.02 at 3 GHz, 4.04 at 5 GHz Dissipation factor DF: 0.0067 at 1 GHz, 0.0059 at 3 GHz, 0.0056 at 5 GHz

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.76 g/cc1.76 g/ccASTM D 792
Linear Mold Shrinkage 0.0015 cm/cm
@Thickness 3.20 mm
0.0015 in/in
@Thickness 0.126 in
ASTM D 955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 123 MPa17900 psiASTM D 638
Elongation at Break 2.0 - 3.0 %2.0 - 3.0 %ASTM D 638
Tensile Modulus 12.4 GPa1800 ksiASTM D 638
Flexural Strength 165 MPa24000 psiASTM D 790
Flexural Modulus 12.4 GPa1800 ksiASTM D 790
Izod Impact, Notched 2.08 J/cm
@Thickness 3.20 mm
3.90 ft-lb/in
@Thickness 0.126 in
ASTM D 256
Izod Impact, Unnotched 7.47 J/cm
@Thickness 3.20 mm
14.0 ft-lb/in
@Thickness 0.126 in
ASTM D 4812
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 3.8
@Frequency 1e+6 Hz
3.8
@Frequency 1e+6 Hz
Dry; ASTM D 150
Dissipation Factor 0.030
@Frequency 1e+6 Hz
0.030
@Frequency 1e+6 Hz
Dry; ASTM D 150
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 5.94 µm/m-°C3.30 µin/in-°FASTM E 831
CTE, linear, Transverse to Flow 64.8 µm/m-°C36.0 µin/in-°FASTM E 831
Deflection Temperature at 0.46 MPa (66 psi) 277 °C530 °FASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 235 °C455 °FASTM D 648
Flammability, UL94 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 327 - 360 °C620 - 680 °F
Mold Temperature 65.6 - 121 °C150 - 250 °F
Drying Temperature 149 °C
@Time 28800 sec
300 °F
@Time 8.00 hour
Dew Point -28.9 °C-20.0 °F
Injection Pressure 82.7 - 124 MPa12000 - 18000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese VECTRA E845i LDS LCP, 40% Mineral / Glass Reinforced
RTP Company RTP 3499-3 X 113393 C Liquid Crystal Polymer (LCP) Glass Fiber - LDS Platable
Celanese VECTRA E840i LDS LCP, 40% Mineral Reinforced
Electrolytic Tough Pitch (ETP) Copper, UNS C11000, H00 Temper flat products
Copper, Cu; Annealed

PQZWA9757 / 92508

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.