MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Vicone High Performance Rubber VicoSil™ 139DLK-BL High Performance Silicone Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone; Silicone Rubber

Material Notes: FDA Approved

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.19 g/cc0.0430 lb/in³ASTM D297
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 4040ASTM D2240
Tensile Strength 7.20 MPa1040 psiASTM D412
Elongation at Break 545 %545 %ASTM D412
Compressive Modulus  0.00180 GPa
@Strain 5.0 %
0.261 ksi
@Strain 5.0 %
ISO-7743
 0.00190 GPa
@Strain 10 %
0.276 ksi
@Strain 10 %
ISO-7743
 0.00220 GPa
@Strain 20 %
0.319 ksi
@Strain 20 %
ISO-7743
 0.00260 GPa
@Strain 25 %
0.377 ksi
@Strain 25 %
ISO-7743
Compression Set 20 %20 %ASTM D395
Tensile Set 6.0 %6.0 %ASTM D412
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
 
Descriptive Properties
ColorBlue
Effect of Liquids - Change in Elongation (%)-12.1ASTM D471
Effect of Liquids - Change in Hardness (%)-5ASTM D471
Effect of Liquids - Change in Tensile Strength (%)-6.3ASTM D471
Effect of Liquids - Change in Volume after Oil Immersion (%)7.7ASTM D471
Heat Aging - Change in Elongation (%)-36ASTM D573
Heat Aging - Change in Hardness (%)6ASTM D573; 200°C; 72h
Heat Aging - Change in Tensile Strength (%)-21.42ASTM D573

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Epoxy Encapsulant, Unreinforced
Vicone High Performance Rubber VicoSil™ 159DLK-RD High Performance Silicone Rubber
Aearo E-A-R Specialty Composites VersaDamp™ V-2325 TPE
Vicone High Performance Rubber VicoSil™ 139DLK-CL High Performance Silicone Rubber
BIW Silicone Rubber Extrusions, Standard Grades

PAVICON990 / 108910

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.