MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Petrothene® GA601031 Linear Low Density Polyethylene
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Injection Molded

Material Notes: Applications
PETROTHENE® GA 601 series are pelletized, linear low density polyethylenes for applications requiring maximum strength and toughness. These products offer excellent additive homogeneity, require no transfer equipment modifications, and facilitate clean and safe handling. Applications include heavy duty shipping sacks, prime liners, commercial and industrial packaging, as well as food and consumer packaging.

Processing Techniques
Recommended processing conditions for the GA 601 series are a 400°-450°F melt temperature and a 1.5-3.01:1 blow-up ratio. Using proper techniques, this product can readily be drawn below 0.9 mil at optimum production rates. Specific recommendations for type of resin and extrusion conditions can be made only when the end use, required properties and processing equipment are known.

Regulatory Status
GA 601 series resins meet the requirements of the Food and Drug

This product is from the former Equistar product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.918 g/cc0.0332 lb/in³ASTM D1505
Thickness 38.1 microns1.50 mil2.5:1 BUR
Melt Flow 1.0 g/10 min1.0 g/10 minASTM D1238
Slip Level 0.000 ppm0.000 ppm
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 550 %550 %ASTM D882
Film Elongation at Break, TD 625 %625 %ASTM D882
Dart Drop, Total Energy 2.44 J1.80 ft-lbASTM D4272
Elmendorf Tear Strength MD 600 g600 gASTM D1922
Elmendorf Tear Strength TD 900 g900 gASTM D1922
Dart Drop Test 290 g0.639 lbF50; ASTM D1709A
Film Tensile Strength at Break, MD 36.5 MPa5300 psiASTM D882
Film Tensile Strength at Break, TD 29.0 MPa4200 psiASTM D882
1% Secant Modulus, MD 207 MPa30000 psiASTM D882
1% Secant Modulus, TD 238 MPa34500 psiASTM D882
 
Optical PropertiesMetricEnglishComments
Haze 12 %12 %ASTM D1003
Gloss 50 %50 %45°; ASTM D2457
 
Descriptive Properties
AntiblockHigh

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Petrothene® GA601030 Linear Low Density Polyethylene
LyondellBasell Petrothene® GA601033 Linear Low Density Polyethylene
LyondellBasell Petrothene® GA601032 Linear Low Density Polyethylene
LyondellBasell Petrothene® NA235000X01 Low Density Polyethylene, Injection Molding Grade
LyondellBasell Petrothene® NA204000 Low Density Polyethylene

PEQU0353a / 36794

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.