MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Park Aerospace Nelcote® E-722 Epoxy Prepreg, 7781 E-Glass Reinforced
Categories: Polymer; Thermoset; Epoxy

Material Notes: Nelcote® E-722 is a modified 350°F cure epoxy system with excellent processing characteristics for vacuum bag, press, and autoclave molding.

Key Features and Benefits:

  • Epoxy resin system optimized for use with woven aramid reinforcements
  • Meets requirements of MIL-R-9300B, Type 1
  • Long out-time for easy processing

Applications/Qualifications:

  • Military Helicopters
  • Engine Nacelles
  • Work Platforms
  • Doors
  • Air Frames

Information provided by Park Electrochemical Corp.

Key Words: EP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles <= 2.0 %
@Temperature 135 °C
<= 2.0 %
@Temperature 275 °F
8 min
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 372 MPa
@Temperature 23.9 °C
54000 psi
@Temperature 75.0 °F
0° Direction, Dry; ASTM D638 Type 1
Tensile Modulus 20.7 GPa
@Temperature 23.9 °C
3000 ksi
@Temperature 75.0 °F
0° Direction, Dry; ASTM D638 Type 1
Flexural Strength 758 MPa
@Temperature 23.9 °C
110000 psi
@Temperature 75.0 °F
Dry; ASTM D790
Flexural Modulus 24.8 GPa
@Temperature 23.9 °C
3600 ksi
@Temperature 75.0 °F
Dry; ASTM D790
Compressive Strength 414 MPa
@Temperature 23.9 °C
60000 psi
@Temperature 75.0 °F
Dry; ASTM D695
Compressive Modulus 20.7 GPa
@Temperature 23.9 °C
3000 ksi
@Temperature 75.0 °F
Dry; ASTM D695
Shear Strength 46.9 MPa
@Temperature 23.9 °C
6800 psi
@Temperature 75.0 °F
Short-Beam, Dry; ASTM D2344
 
Processing PropertiesMetricEnglishComments
Gel Time 1.00 - 2.50 min1.00 - 2.50 min
Shelf Life 12.0 Month
@Temperature -17.8 °C
12.0 Month
@Temperature 0.000 °F
 
Descriptive Properties
Prepreg Resin Content (%)35-40
Resin Flow (%)7-21325°F, 15psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AGY ADVANTEX® Generic Glass Fiber
E-CRGlas® Fiber
E-Glass Fiber, Generic
Park Aerospace Nelcote® V-376 Cyanate Ester Epoxy Prepregs, 7781 E-Glass Reinforced
Park Aerospace Nelcote® E-746 Epoxy Prepreg, 7781 E-Glass Reinforced

PPARK007 / 89279

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.