MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M 4317 Single-Coated Foam Tape
Categories: Polymer; Tape

Material Notes: 3M™ Single-Coated Foam Tapes will adhere to a variety of substrates, including latex-painted wood, lacquered wood, enameled steel, glass, aluminum, stainless steel, acrylic, ABS, and PVC (non-plasticized) as tape adhesion is typically satisfactory within 20 minutes and continues to build and additional time.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.0320 g/cc0.00116 lb/in³foam with adhesive; ASTM D3574
Thickness 76.2 microns3.00 milRelease Liner
 9530 microns375 milTotal
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore OO 6.06.0Foam with adhesive; ASTM D2240
Tensile Strength at Break 0.170 MPa24.7 psiDie "A"; ASTM D3759
Elongation at Break 125 %125 %Die "A"; ASTM D3759
Compressive Strength 0.00207 MPa0.300 psiDeflection, Compress 25%; ASTM D3574
Compression Set 5.0 %5.0 %ASTM D1667
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 3.00e+12 ohm3.00e+12 ohmNon-adhesive side; ASTM D257
 5.00e+12 ohm5.00e+12 ohmAdhesive side; ASTM D257
Dielectric Strength 1.57 kV/mm40.0 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.0430 W/m-K0.298 BTU-in/hr-ft²-°FASTM C518
 
Descriptive Properties
Adhesive Type430
AppearanceCharcol gray
 Tanliner

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M 4317 Foam Tape
Mid-Mountain Materials CERMEX® PR1000-C Commercial Grade Thermal Insulation Paper
Northstar Polymers MPP-F07A Easy Hand-Mixable/Pourable Flexible Foam
Eurofoam Porocell POR 304 B-OPC EPDM Foam
Dow 3-6651 THERMALLY CONDUCTIVE ELASTOMER, KIT

PMM34561 / 169308

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.