MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LATI Lastilac 10 ABS/PC
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced

Material Notes: ABS/PC Blend (ABS/PC). Unfilled. Very good surface appearance. High impact resistance. Good thermal properties.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Information provided by Lati Industria Termoplastici S.p.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.12 g/cc0.0405 lb/in³
Linear Mold Shrinkage, Flow 0.0055 - 0.0075 cm/cm0.0055 - 0.0075 in/in
Linear Mold Shrinkage, Transverse 0.0055 - 0.0075 cm/cm0.0055 - 0.0075 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break  20.0 MPa
@Temperature 90.0 °C
2900 psi
@Temperature 194 °F
 45.0 MPa
@Temperature 60.0 °C
6530 psi
@Temperature 140 °F
 55.0 MPa
@Temperature 23.0 °C
7980 psi
@Temperature 73.4 °F
Elongation at Break  40 %
@Temperature 23.0 °C
40 %
@Temperature 73.4 °F
 45 %
@Temperature 60.0 °C
45 %
@Temperature 140 °F
 55 %
@Temperature 90.0 °C
55 %
@Temperature 194 °F
Elongation at Yield  4.0 %
@Temperature 60.0 °C
4.0 %
@Temperature 140 °F
 5.0 %
@Temperature 23.0 °C
5.0 %
@Temperature 73.4 °F
 6.0 %
@Temperature 90.0 °C
6.0 %
@Temperature 194 °F
Tensile Modulus  1.90 GPa
@Temperature 90.0 °C
276 ksi
@Temperature 194 °F
 2.20 GPa
@Temperature 60.0 °C
319 ksi
@Temperature 140 °F
 2.50 GPa
@Temperature 23.0 °C
363 ksi
@Temperature 73.4 °F
Charpy Impact Unnotched NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
Charpy Impact, Notched 6.50 J/cm²
@Temperature 23.0 °C
30.9 ft-lb/in²
@Temperature 73.4 °F
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 250 V250 VA solution
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 75.0 °C167 °F
Deflection Temperature at 0.46 MPa (66 psi) 110 °C230 °F
Deflection Temperature at 1.8 MPa (264 psi) 105 °C221 °F
Vicat Softening Point 110 °C
@Load 5.00 kg
230 °F
@Load 11.0 lb
Oxygen Index 25 %25 %
 
Processing PropertiesMetricEnglishComments
Melt Temperature 230 - 250 °C446 - 482 °F
Mold Temperature 50.0 - 70.0 °C122 - 158 °F
Drying Temperature 80.0 - 100 °C
@Time 10800 sec
176 - 212 °F
@Time 3.00 hour
 
Descriptive Properties
ISO Shrinkage - Pressure60 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LATI LASTILAC 11 G/20-V0 20% Glass Fiber Reinforced ABS/PC-Based Alloy
A. Schulman Diamond ABS/PC 7901
Daicel CEVIAN® S5220 20% GF PC/ABS alloy
MRC Polymers NAXALOY™ 770-NT172 ABS + PC Alloy
RTP Company RTP 687 FR  Acrylonitrile Butadiene Styrene (ABS) Carbon Fiber 40% - Flame Retardant

PLATH9664 / 177360

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.