MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil Santoprene® 151-70W256 Thermoplastic Vulcanizate - Flame Retardant
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Product Description: A soft, black, flame retardant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material has been designed to meet the Underwriter Laboratories (UL) Subjects 6703, UL 6703A and UL 1703 material requirements for both junction boxes and connectors (both enclosure and insulation) for use in photovoltaic systems. The flame retardants used are RoHS compliant and provide UL 94 flammability classifications of V-1 down to a thickness of 1.5 mm and 5VA down to a thickness of 1.8 mm. The material has an elevated Relative Thermal Index (RTI) of 90°C and meets the requirements for suitability for outdoor use with an (f1) rating. This grade of Santoprene TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding. It is polyolefin based and completely recyclable.

Key Features:

  • Suitability for outdoor use.
  • EU and China RoHS compliant.
  • UL listed: file #QMFZ2.E80017, Plastics - Component; file #QMFZ8.E80017, Plastics Certified For Canada - Component.
Availability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South America

Information provided by ExxonMobil Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.26 g/cc1.26 g/ccASTM D792 and ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 75752 mm; ISO 868
Tensile Strength at Break 4.80 MPa696 psiAcross Flow; ASTM D412 and ISO 37
Tensile Stress at Strain 2.30 MPa
@Strain 100 %
334 psi
@Strain 100 %
Across Flow; ASTM D412 and ISO 37
Elongation at Break 480 %480 %Across Flow; ASTM D412 and ISO 37
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 28.3 kV/mm
@Thickness 2.03 mm
720 kV/in
@Thickness 0.0799 in
ASTM D149
 
Thermal PropertiesMetricEnglishComments
UL RTI, Electrical 90.0 °C194 °FUL 746
UL RTI, Mechanical without Impact 90.0 °C194 °FUL 746
Flammability, UL94  V-1
@Thickness 1.50 - 3.00 mm
V-1
@Thickness 0.0591 - 0.118 in
UL File Number - E80017
 5VA
@Thickness 1.80 mm
5VA
@Thickness 0.0709 in
 5VA
@Thickness 3.00 mm
5VA
@Thickness 0.118 in
Oxygen Index 24 %24 %ASTM D2863 and ISO 4589-2
 
Descriptive Properties
Inclined Plane Tracking107 minUL 746/ASTM D2303
Outdoor Suitabilityf1UL 746C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil Santoprene® 101-64 Thermoplastic Elastomer
ExxonMobil Santoprene® 101-80 Thermoplastic Elastomer
ExxonMobil Santoprene® 151-60 Thermoplastic Rubber
ExxonMobil Santoprene® 251-80W232 Thermoplastic Elastomer
ExxonMobil Santoprene® 121-70M350 Thermoplastic Vulcanizate - UV Resistant

PEXA912 / 125955

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.