MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Indorama Ventures Mexico Polyclear™ Preserve 2201 PET Resin
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), Unreinforced

Material Notes: Description: La resina Polyclear® Preserve PET 2201 de Arteva Specialties, es un copolimero para empaque con una viscosidad intrinseca de 0.84 dl/g y esta disenada para ofrecer un redimiento superior en envases para aplicaciones de llenado en caliente y pasteurizacion. Los envases fabricados con resina Polyclear® Preserve PET 2201 tienen excelente claridad y destacan por su estabilidad dimensional que impide la contraccion y espansion; incluso al tratamiento termico posterior al llenado. La resina Polyclear® Preserve PET 2201 es usada exitosamente en botellas para procesos de “Heat Set” y “Hot Fill” para jugos, tes, bebidas isotonicas y alimentos. La resina Polyclear® Preserve PET 2201 tambien se utiliza con exito en botellas pasteurizables para cerveza, bebidas alcoholicas saborizadas y otros bebidas carbonatadas. La resina cumple con la regulacion de la Federal Food, Drug and Cosmetic Act para aplicaciones especificas en alimentos. Para mayores detalles de la FDA, por favor contacte a Arteva Specialties. Los envases elaborados con la resina PET de Arteva Specialties son ligeros, irrompibles, tienen excelentes propiedades de barrera. Son atoxicos, se pueden pigmentar en una amplia gama de colores, y tienen la gran ventaja de ser totalmente reciclables.

Key Words: Excellent clarity and dimensional stability
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density >= 1.394 g/cc>= 0.05036 lb/in³Limit; M2E-71-043
 1.398 g/cc0.05051 lb/in³Target; M2E-71-043
Apparent Bulk Density 0.880 g/cc0.0318 lb/in³Target; M2E-72-015
 0.830 - 0.930 g/cc0.0300 - 0.0336 lb/in³Limit; M2E-72-015
Viscosity Measurement 0.820.82Target; M2E-75-011
 0.80 - 0.840.80 - 0.84Limits; M2E-75-011
Crystallinity >= 50 %>= 50 %Limit; M2E-71-043
 53 %53 %Target; M2E-71-043
 
Chemical PropertiesMetricEnglishComments
Acetaldehyde 0.500 ppm0.500 ppmTarget; M2E-75-007
 <= 1.50 ppm<= 1.50 ppmLimit; M2E-75-007
 
Thermal PropertiesMetricEnglishComments
Melting Point 238 °C460 °FTarget; M2E-73-002
 230 - 246 °C446 - 475 °FLimits; M2E-73-002
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %clear; thickness not quantified
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.10 %<= 0.10 %M2E-72-010
 
Descriptive Properties
Chip Size55 - 65 No/gLimits, M2E-75-004
 60 No/gTarget, M2E-75-004
Color, CIE-2.0 (b)Target, M2E-75-002
 -3.5 to -0.5 (b)Limits, M2E-75-002
Fines< 0.1%M2E-76-033
ProcessBlow Molding
 Injection Molding
Yellow Chips< 9 No/125gM2E-75-014

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Indorama Auriga Polymers Polyclear™ Perserve 2201 PET Resin
UBE 7128B Nylon 6/12 Copolymer
Indorama AlphaPet Preformance® ES11(A) PET Resin
Indorama AlphaPet Preformance® 1708HS(A) PET Resin
Indorama AlphaPet Preformance® 1708CC(A) PET Resin

PINDOM911 / 126385

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.