MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Petrothene® NA362176 Low Density Polyethylene  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: Applications
PETROTHENE NA 362 is a series of low density/EVA copolymers designed for ice bags, bag-in-box, heavy-duty skin packaging and other high strength, easy to seal packaging. NA 362 exhibits high impact strength and good low temperature toughness.

Regulatory Status
The base resin NA 362 meets the requirements of the Food and Drug Administration regulation 21 CFR 177.1350. This regulation allows the use of this ethylene vinyl acetate copolymer "…in articles or components of articles intended for use in contact with food." Specific limitations or conditions of use may apply.

Processing Techniques
Specific recommendations for processing NA 362 can only be made when the processing conditions, equipment and end use are known.

Physical Properties
These are typical values and not to be construed as specific product limits. Data obtained fro

This product is from the former Equistar product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.926 g/cc0.0335 lb/in³ASTM D1505
Vinyl Acetate Content 6.6 %6.6 %
Thickness 50.8 microns2.00 mil2:1 BUR; 25 mil die gap
Melt Flow 0.50 g/10 min0.50 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 500 %500 %ASTM D882
Film Elongation at Break, TD 600 %600 %ASTM D882
Elmendorf Tear Strength MD 140 g140 gASTM D1922
Elmendorf Tear Strength TD 260 g260 gASTM D1922
Dart Drop Test 310 g0.684 lbF50; ASTM D1709
Film Tensile Strength at Break, MD 26.2 MPa3800 psiASTM D882
Film Tensile Strength at Break, TD 24.8 MPa3600 psiASTM D882
1% Secant Modulus, MD 117 MPa17000 psiASTM D882
1% Secant Modulus, TD 145 MPa21000 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 87.0 °C189 °FASTM D1525
 
Processing PropertiesMetricEnglishComments
Melt Temperature 221 °C430 °F
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
AntiblockHigh
SlipHigh

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Alathon® M5370 High Density Polyethylene
LyondellBasell Petrothene® NA362005 Low Density Polyethylene
LyondellBasell Petrothene® NA960000 Low Density Polyethylene
LyondellBasell Petrothene® NA963083 Low Density Polyethylene
LyondellBasell Petrothene® NA940094 Low Density Polyethylene (Film Grade)

PEQU0486a / 36939

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.