MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Bakelite® PF 51 Phenolic Formaldehyde Resin, Special Preparation Cylindrical Pellets
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic

Material Notes: Phenolic molding compound, organically filled, reinforced with cotton fibers, increased notched impact strength.

Applications: contactor cross bar, MCB housings, handwheels.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.42 g/cc0.0513 lb/in³ISO 1183
Apparent Bulk Density 0.600 g/cc0.0217 lb/in³ISO 60
Linear Mold Shrinkage 0.0050 cm/cm0.0050 in/inCompression Molding. Post Shrinkage = 0.55%.; ISO 2577
 0.0080 cm/cm0.0080 in/inInjection Molding. Post Shrinkage = 0.5%.; ISO 2577
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 280 MPa40600 psiH961/30; ISO 2039/P1
Flexural Strength 90.0 MPa13100 psiISO 178
Flexural Modulus 8.00 GPa1160 ksiISO 178
Compressive Strength 225 MPa32600 psiISO 604
Charpy Impact Unnotched 0.700 J/cm²3.33 ft-lb/in²ISO 179-1 eU
Charpy Impact, Notched 0.270 J/cm²1.28 ft-lb/in²ISO 179-1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+11 ohm-cm1.00e+11 ohm-cm
Surface Resistance 1.00e+10 ohm1.00e+10 ohm
Dielectric Constant 17.5
@Frequency 100 Hz
17.5
@Frequency 100 Hz
Dielectric Strength 10.5 kV/mm
@Thickness 1.00 mm
267 kV/in
@Thickness 0.0394 in
IEC 60243-P1
Dissipation Factor 0.25
@Frequency 100 Hz
0.25
@Frequency 100 Hz
Comparative Tracking Index 125 V125 V
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 130 °C266 °F<20000 hours; IEC 60216-P1
 160 °C320 °F< 50 hours; IEC 60216-P1
Deflection Temperature at 8.0 MPa 120 °C248 °FISO 75-2
 
Processing PropertiesMetricEnglishComments
Feed Temperature 60.0 - 75.0 °C140 - 167 °FInjection molding
Nozzle Temperature 80.0 - 100 °C176 - 212 °FInjection molding
Melt Temperature 80.0 - 100 °C176 - 212 °FInjection molding
Mold Temperature 160 - 190 °C320 - 374 °FInjection molding
 160 - 190 °C320 - 374 °FCompression molding
Injection Pressure >= 15.0 MPa>= 2180 psiCompression and injection cavity mold pressure
Back Pressure 0.500 - 2.00 MPa72.5 - 290 psiInjection molding
Cure Time 0.167 - 0.333 min0.00278 - 0.00556 hourPer 1 mm of wall thickness, injection molding
 0.333 - 0.667 min0.00556 - 0.0111 hourPer 1 mm of wall thickness, compression molding
 
Descriptive Properties
Chromatic SpectrumSubdued Colors
Creep Rupture StrengthGood
Holding PressureApproximately 40-60% of injection pressure
Media ResistanceGood
Thermal ExpansionSlight
Water absorption (mg)8524h / 23°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Bakelite® PF 6501 Phenolic Formaldehyde Resin, Low Shrinkage
Bakelite® PF 31 Phenolic Formaldehyde Resin, UL Listed
Bakelite® MP 4165 Melamine Phenolic Resin, Copper Adhesive, Low Shrinkage, High Mechanical Strength
Bakelite® PF 85 Phenolic Formaldehyde Resin, UL Listed
Chosun Refractories MF-2 Blast Furnace Tap-Hole Refractory

PBAKE007 / 27041

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.