MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Atom Adhesives AA-BOND F110 Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: AA-BOND F110 is a rigid, optically clear adhesive with a very low viscosity. AA-BOND F110 is room temperature system an excellent choice for thin bond-line assembly and repair applications of prisms, lenses and other optic components. And its high strength makes this epoxy ideal for structural applications. AA-BOND F110 exhibits excellent wetting and wicking capabilities which allows it to adhere strongly to glass, ceramics, metals and most rigid plastics.

Appearance: Transparent, Clear

Cure Type: Heat cure or Room Temperature

Benefits:

  • High strength
  • Perfect insulative properties
  • Good resistance to salt solutions, mold acids and Alkalis and many other chemicals
Mix Ratio by weight: 100:100/Resin:Hardener

Substrates: Excellent choice for thin bond-line assembly and repair applications of prisms, lenses and other optic components.

Typical Application: Exhibits excellent wetting and wicking capabilities which allows it to adhere strongly to glass, ceramics, metals and most rigid plastics.

Information provided by Atom Adhesives

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.16 g/cc1.16 g/ccuncured
Solids Content 100 %100 %reactive, uncured
Volatile Organic Compounds (VOC) Content 39.1 g/l39.1 g/luncured
Viscosity 310 cP310 cPuncured
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8383
Shear Strength  14.8 MPa
@Temperature 25.0 °C,
Time 86400 sec
2150 psi
@Temperature 77.0 °F,
Time 24.0 hour
Lap, Alum to Alum
 17.9 MPa
@Temperature 65.0 °C,
Time 3600 sec
2600 psi
@Temperature 149 °F,
Time 1.00 hour
Lap, Alum to Alum
 20.7 MPa
@Temperature 65.0 °C,
Time 14400 sec
3000 psi
@Temperature 149 °F,
Time 4.00 hour
Lap, Alum to Alum
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 6.00e+13 ohm-cm6.00e+13 ohm-cm
Dielectric Constant 4.3
@Frequency 1000 Hz
4.3
@Frequency 1000 Hz
Dielectric Strength 16.1 kV/mm410 kV/in
 
Thermal PropertiesMetricEnglishComments
CTE, linear 59.9 µm/m-°C33.3 µin/in-°F
Maximum Service Temperature, Air 130 °C266 °F
Minimum Service Temperature, Air -60.0 °C-76.0 °F
Glass Transition Temp, Tg 90.0 °C194 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.541.54
Transmission, Visible 97 %97 %
 
Processing PropertiesMetricEnglishComments
Cure Time  60.0 - 120 min
@Temperature 65.0 °C
1.00 - 2.00 hour
@Temperature 149 °F
 1440 min
@Temperature 25.0 °C
24.0 hour
@Temperature 77.0 °F
Pot Life 30.0 min30.0 minuncured
 
Descriptive Properties
Thixotropic Index1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Arlon Electronic Materials 45N Multifunctional Epoxy Laminate and Prepreg
Atom Adhesives AA-BOND 2110 Epoxy Adhesive
Atom Adhesives AA-BOND F113 Epoxy Adhesive
Abatron AboGlass-1 Epoxy Decoupage Resin
Aremco Aremco-Bond™ 2330 High Performance Epoxide

PATOM016 / 172331

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.