MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Arkema KYNAR FLEX® 2850 PC Polyvinylidene Fluoride Spray Coating Powder
Categories: Polymer; Thermoplastic; Fluoropolymer; Polyvinylidene Fluoride (PVDF); Polyvinylidinefluoride (PVDF), Molded/Extruded

Material Notes: Electrostatic spray

Information provided by Arkema Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.77 - 1.80 g/cc1.77 - 1.80 g/ccASTM D792
Density 1.78 g/cc0.0643 lb/in³ISO 1183
Water Absorption 0.030 %0.030 %Dry; Sim. to ISO 62
Viscosity 400000 - 800000 cP
@Shear Rate 100 1/s,
Temperature 230 °C
400000 - 800000 cP
@Shear Rate 100 1/s,
Temperature 446 °F
Melt; ASTM D3835
Melt Flow  7.5 g/10 min
@Load 3.80 kg,
Temperature 230 °C
7.5 g/10 min
@Load 8.38 lb,
Temperature 446 °F
cm³/10 min Volumetric Rate; ISO 1133
 8.0 - 25 g/10 min
@Load 3.80 kg,
Temperature 230 °C
8.0 - 25 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 70 - 7570 - 75ASTM D2240
Tensile Strength at Break 27.6 - 48.3 MPa4000 - 7010 psiASTM D638
Tensile Strength, Yield 35.0 MPa5080 psiDry; ISO 527-1/-2
 31.0 - 41.4 MPa4500 - 6000 psiASTM D638
Elongation at Break >= 50 %>= 50 %Dry; ISO 527-1/-2
 30 - 200 %30 - 200 %ASTM D638
Elongation at Yield 5.0 - 15 %5.0 - 15 %ASTM D638
 10 %10 %Dry; ISO 527-1/-2
Tensile Modulus 1.03 - 1.52 GPa149 - 220 ksiASTM D638
Flexural Strength 20.7 - 27.6 MPa
@Strain 5.0 %
3000 - 4000 psi
@Strain 5.0 %
ASTM D790
Flexural Modulus 1.03 - 1.24 GPa149 - 180 ksiASTM D790
Compressive Strength 41.4 - 586 MPa6000 - 85000 psiASTM D695
Izod Impact, Notched 1.60 - 4.27 J/cm3.00 - 8.00 ft-lb/inASTM D256
Izod Impact, Unnotched NBNBASTM D256
Coefficient of Friction, Dynamic 0.190.19vs. steel; ASTM D1894
Coefficient of Friction, Static 0.260.26vs. steel; ASTM D1894
Taber Abrasion, mg/1000 Cycles 6.0 - 9.06.0 - 9.0CS 17 1000g:pad; ASTM-G195-13A
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.00e+14 ohm-cm2.00e+14 ohm-cm65% R.H; ASTM D257
 2.00e+14 ohm-cm2.00e+14 ohm-cmDry; IEC 60093
Dielectric Constant 3.5 - 10.2
@Frequency 1000 Hz
3.5 - 10.2
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 1.30 - 1.60 kV/mm33.0 - 40.6 kV/inASTM D149
Dissipation Factor 0.010 - 0.22
@Frequency 100000 Hz
0.010 - 0.22
@Frequency 100000 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 126 - 185 µm/m-°C70.0 - 103 µin/in-°FASTM D696
Specific Heat Capacity 0.745 - 0.958 J/g-°C0.178 - 0.229 BTU/lb-°FDSC
Thermal Conductivity 0.144 - 0.180 W/m-K0.999 - 1.25 BTU-in/hr-ft²-°FASTM D433
Melting Point 155 - 160 °C311 - 320 °FASTM D3418
 158 °C316 °F10°C/min; Dry; ISO 11357-1/-3
Maximum Service Temperature, Air 140 °C284 °FUL RTI
Deflection Temperature at 0.46 MPa (66 psi) 60.0 - 75.0 °C140 - 167 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 46.0 °C115 °FDry; ISO 75-1/-2
 37.8 - 55.0 °C100 - 131 °FASTM D648
Glass Transition Temp, Tg -40.6 - -38.3 °C-41.1 - -36.9 °FASTM D7028
Decomposition Temperature 375 °C707 °F1% wt. loss, TGA, in air
 410 °C770 °F1% wt. loss, TGA, in nitrogen
Flammability, UL94 V-0
@Thickness 0.800 mm
V-0
@Thickness 0.0315 in
IEC 60695-11-10
Oxygen Index 43 %43 %ASTM D2863
 43 %43 %Dry; ISO 4589-1/-2
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.421.42sodium D line; ASTM D542
 
Descriptive Properties
Moisture SensitiveNo

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Arkema Kynar Flex® 2821-00 Polyvinylidene Fluoride Powder
Arkema Kynar Flex® 2801-00 Polyvinylidene Fluoride Powder
Arkema Kynar Flex® 2751-00 Polyvinylidene Fluoride Powder
Aremco Corr-Paint™ CP2050-XX High Temperature Protective Coating Epoxy-Phenolic, Glass Fiber Filled
Arkema Kynar® 710 Polyvinylidene Fluoride Homopolymer- Injection Molding

PARKG942 / 144567

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.