MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

A. Schulman ComAlloy Hiloy® 152 Polypropylene, Mineral Reinforced
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Mineral Reinforced

Material Notes: Data provided by the manufacturer, ComAlloy International Company.

20% Mineral Reinforced.

The ComAlloy product line has been integrated into the A Schulman product line.

Key Words: ComAlloy International Company, subsidiary of A. Shulman Inc.
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.07 g/cc0.0387 lb/in³
Linear Mold Shrinkage 0.015 cm/cm0.015 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 9898ASTM D785
Tensile Strength, Ultimate 17.0 MPa2470 psiASTM D638
Elongation at Break 74.3 %74.3 %ASTM D638
Flexural Strength 49.0 MPa7110 psiASTM D790
Flexural Modulus 2.10 GPa305 ksiASTM D790
Izod Impact, Notched 0.210 J/cm0.393 ft-lb/inASTM D256
Izod Impact, Unnotched 5.60 J/cm10.5 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 118 °C244 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 69.0 °C156 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Middle Barrel Temperature 210 - 221 °C410 - 430 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A.D. Compound Adene NC180A Homopolymer 15% CaCO3 Filled Polypropylene
Aclo Accutech Polypropylene Copolymer HP0334W30L Wollastonite Reinforced
Buckeye Polymers BP RPP 1510 C Polypropylene, 15% Mineral Filled
Overview of materials for Polypropylene, Mineral Reinforced
RTP Company RTP 132 Polypropylene (PP), Talc

PASH2U / 24865

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.