MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

E-Polymers TEKASTER® F101F Fast cycle time PBT
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: Injection molding. PBT has excellent mechanical properties and well balanced engineering plastics with an electrical performance. Specially G/F reinforced PET has excellent heat resistance, a good surface, chemical resistance and high electrical performance.

Information Provided by E-Polymers Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.31 g/cc1.31 g/ccASTM D792
Linear Mold Shrinkage 0.016 cm/cm0.016 in/in
Linear Mold Shrinkage, Transverse 0.030 cm/cm0.030 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 54.936 MPa7967.8 psiASTM D638
Elongation at Break 100 %100 %ASTM D638
Flexural Strength 78.48 MPa11380 psiASTM D790
Flexural Modulus 2.1582 GPa313.02 ksiASTM D790
Izod Impact, Notched 0.343 J/cm0.643 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 155 °C311 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 57.0 °C135 °FASTM D648
Flammability, UL94 HBHB
 
Processing PropertiesMetricEnglishComments
Melt Temperature 230 - 250 °C446 - 482 °F
Mold Temperature 40.0 - 60.0 °C104 - 140 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
E-Polymers Tekaloy® T80 , Dimensional Stability PBT/ABS Alloy
E-Polymers Tekaloy® T80HI Impact Resistance PBT/ABS Alloy
E-Polymers TEKASTER® F101M Unreinforced impact modified PBT
E-Polymers TEKASTER® F100 low-mid viscosity PBT
Epsan Epimix PBT-PET GV0 30 NC Q1D001 Polybutylene Terephthalate/Polyethylene terephthalate

PEPOLZ023 / 103520

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.