MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Domo TECHNYL® C 548B V15 Black PA6, 15% glass filled, DRY
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 20% Glass Fiber Filled

Material Notes: Description: Polyamide PA6, reinforced with 15% of glass fiber, heat stabilized, height viscosity, for extrusion-blowing.

Available in: Asia Pacific and North America

Product Applications: TECHNYL C 548B V15 is suitable in the automotive industry for blow-molded parts, mainly in the oil and air circuits, such as: air intake ducts, turbo to intercooler pipe, intercooler exit duct. This product is available in black.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.18 g/cc0.0426 lb/in³ISO 1183/A
Water Absorption 1.42 %
@Temperature 23.0 °C,
Time 86400 sec
1.42 %
@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 85.0 MPa12300 psiISO 527 Type 1A
Elongation at Break 3.0 %3.0 %ISO 527 Type 1A
Tensile Modulus 5.00 GPa725 ksiISO 527 Type 1A
Izod Impact, Notched (ISO) 14.0 kJ/m²6.66 ft-lb/in²ISO 180/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohm1.00e+13 ohmIEC 60093
Dielectric Constant 3.73.7IEC 60250
Dissipation Factor 0.0200.020IEC 60250
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 40.0 µm/m-°C
@Temperature 23.0 - 85.0 °C
22.2 µin/in-°F
@Temperature 73.4 - 185 °F
ISO 11359
Melting Point 222 °C432 °FISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 185 °C365 °FISO 75/Af
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
1210
 
Processing PropertiesMetricEnglishComments
Feed Temperature 200 - 220 °C392 - 428 °F
Adapter Temperature 220 - 240 °C428 - 464 °F
Die Temperature 215 - 235 °C419 - 455 °F
Head Temperature 220 - 240 °C428 - 464 °F
Screw Cooling Temperature 220 - 240 °C428 - 464 °F
Mold Temperature 40.0 - 60.0 °C104 - 140 °F
Drying Temperature 80.0 °C176 °F
Moisture Content <= 0.080 %<= 0.080 %
 
Descriptive Properties
Compression Zone230-240°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
NYCOA 2037 15% Glass Filled Nylon 6
Domo Technyl® C216V15 15% Glass Filled Nylon 6
Domo Technyl® A216V15 15% Glass Filled Nylon 66
BASF Ultramid® S3EG6 Balance 30% Glass Filled PA 610 (Conditioned)
Avient Edgetek® NT-15GF/000 High Impact Nylon 66 - 15% Glass Fiber Reinforced

PRHOD800 / 138031

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.