MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Kraton® G4609 H (SEBS) with Oil  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Description: Kraton G4609 H is a white mineral oil extended linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 33%. Nominal oil content of the polymer is 45.5%w (90 parts/100 parts rubber (phr)). It is supplied from North America in the physical form identified:
Kraton G4609 H supplied as a powder

Region: Asia Pacific, Europe, Japan, North America, and South America

Uses: Kraton G4609 H is used as a base material for thermoplastic elastomer (TPE) compound formulations for a variety of applications. It is also used as a modifier of thermoplastics and bitumen. The inherent stability of SEBS polymers suggests the use of G4609 H in applications that must withstand weathering and high processing temperatures.

Applications: Compounding and Personal Hygiene

Information provided by Kraton®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles <= 1.0 %<= 1.0 %BAM 908
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength >= 4.14 MPa>= 600 psiBAM 1211
 
Descriptive Properties
ContentDust, Calcium Carbonate2-6%, BAM 908
 Non-staining phenolic antioxidant0-0%, BAM 929
 Polystyrene31.2-34.6%, Measured on the polymer before hydrogenation, BAM 919
 Total Extractables43-52%, BAM 1206

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kraton® A1536 H (SEBS) Linear Triblock Copolymer
Kraton® D1193 P (SIS) Linear Triblock Copolymer
Kraton® FG1901 G (SEBS) grafted with MA
Kraton® G1641 H (SEBS) Linear Triblock Copolymer
Kraton® G1651 E (SEBS) Linear Triblock Copolymer

PKRA9914 / 132813

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.