MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

VICTREX™ PEEK 450CA40 Polyetheretherketone, 40% Carbon Fibre Reinforced
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Carbon Fiber Filled

Material Notes: Product Description:

High performance thermoplastic material, 40% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, FDA food contact compliant, colour black.

Typical Application Areas:

Applications for higher strength and stiffness in a static or dynamic system. Excellent wear resistance, low coefficient of friction, low coefficient of thermal expansion. Chemically resistant to aggressive environments.

Information Provided by Victrex.

Vendors: Victrex is a global leader in high-performance PEEK and PAEK polymers, transforming industries from aerospace to medical devices. For 40 years, our innovative polymer solutions help customers achieve new levels of performance, sustainability, and cost efficiency across applications that millions rely on daily from smartphones to aircraft components. As pioneers in polymer engineering, we're committed to delivering transformational solutions that address global materials challenges. Visit www.victrex.com, call (800) VICTREX /1-484-342-6001, or email victrexplc@victrex.com.

Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.44 g/cc0.0520 lb/in³Crystalline; ISO 1183
Water Absorption at Saturation  0.25 %
@Temperature 23.0 °C
0.25 %
@Temperature 73.4 °F
ISO 62-1
 0.45 %
@Temperature 100 °C
0.45 %
@Temperature 212 °F
ISO 62-1
Viscosity 850000 cP
@Temperature 400 °C
850000 cP
@Temperature 752 °F
melt; ISO 11443
Linear Mold Shrinkage, Flow 0.0010 cm/cm0.0010 in/in405°C nozzle, 200°C tool; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0050 cm/cm0.0050 in/in405°C nozzle, 200°C tool; ISO 294-4
Spiral Flow 6.50 cm
@Thickness 1.00 mm
2.56 in
@Thickness 0.0394 in
Mold Temp: 200°C, Melt Temp: 405°C
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8888ISO 868
Tensile Strength at Break  65.0 MPa
@Temperature 275 °C
9430 psi
@Temperature 527 °F
ISO 527
 105 MPa
@Temperature 175 °C
15200 psi
@Temperature 347 °F
ISO 527
 175 MPa
@Temperature 125 °C
25400 psi
@Temperature 257 °F
ISO 527
 285 MPa
@Temperature 23.0 °C
41300 psi
@Temperature 73.4 °F
ISO 527
Elongation at Break 1.5 %
@Temperature 23.0 °C
1.5 %
@Temperature 73.4 °F
ISO 527
Tensile Modulus 35.0 GPa
@Temperature 23.0 °C
5080 ksi
@Temperature 73.4 °F
ISO 527
Flexural Strength  90.0 MPa
@Temperature 275 °C
13100 psi
@Temperature 527 °F
ISO 178
 160 MPa
@Temperature 175 °C
23200 psi
@Temperature 347 °F
ISO 178
 290 MPa
@Temperature 125 °C
42100 psi
@Temperature 257 °F
ISO 178
 380 MPa
@Temperature 23.0 °C
55100 psi
@Temperature 73.4 °F
ISO 178
Flexural Modulus 30.0 GPa
@Temperature 23.0 °C
4350 ksi
@Temperature 73.4 °F
ISO 178
Compressive Strength  60.0 MPa
@Temperature 250 °C
8700 psi
@Temperature 482 °F
ISO 604
 90.0 MPa
@Temperature 200 °C
13100 psi
@Temperature 392 °F
ISO 604
 230 MPa
@Temperature 120 °C
33400 psi
@Temperature 248 °F
ISO 604
 360 MPa
@Temperature 23.0 °C
52200 psi
@Temperature 73.4 °F
ISO 604
Izod Impact, Notched (ISO) 11.0 kJ/m²
@Temperature 23.0 °C
5.23 ft-lb/in²
@Temperature 73.4 °F
ISO 180/A
Izod Impact, Unnotched (ISO) 20.0 kJ/m²
@Temperature 23.0 °C
9.52 ft-lb/in²
@Temperature 73.4 °F
ISO 180/U
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1e+051e+051V; ASTM D4496
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  5.00 µm/m-°C
@Temperature <=143 °C
2.78 µin/in-°F
@Temperature <=289 °F
Below Tg; ISO 11359
 8.00 µm/m-°C
@Temperature >=143 °C
4.44 µin/in-°F
@Temperature >=289 °F
Above Tg; ISO 11359
CTE, linear, Transverse to Flow  35.0 µm/m-°C
@Temperature <=143 °C
19.4 µin/in-°F
@Temperature <=289 °F
Below Tg; ISO 11359
 90.0 µm/m-°C
@Temperature >=143 °C
50.0 µin/in-°F
@Temperature >=289 °F
Above Tg; ISO 11359
Melting Point 343 °C649 °FISO 11357
Glass Transition Temp, Tg 143 °C289 °FOnset; ISO 11357
 150 °C302 °FMidpoint; ISO 11357
Glow Wire Flammability Index 960 °C
@Thickness 2.00 mm
1760 °F
@Thickness 0.0787 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Processing Temperature <= 100 °C<= 212 °FHopper Temperature
Rear Barrel Temperature 380 °C716 °F
Middle Barrel Temperature 380 - 395 °C716 - 743 °F
Front Barrel Temperature 400 °C752 °F
Nozzle Temperature 405 °C761 °F
Mold Temperature 190 - 210 °C374 - 410 °F
Drying Temperature 120 - 150 °C
@Time 10800 - 18000 sec
248 - 302 °F
@Time 3.00 - 5.00 hour
 
Descriptive Properties
Gate>2 mm or 0.5 x part thickness
Runner>3.5mmmanifold
 >3mm Die/nozzle

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Plastcom SLOVAMID 66 CF 30 TS PA 66 reinforced with 30% carbon fibre, thermal stabilization
VICTREX™ PEEK 90HMF40 Polyetheretherketone (PEEK), 40% Carbon Fiber Reinforced
VICTREX™ PEEK 450CA30 30% Carbon Fiber Reinforced
Plastcom SLOVAMID 66 CF 40 PA66, 40% carbon fibre
VICTREX™ PEEK 450CA20 Polyetheretherketone, 20% Carbon Fibre Reinforced

PVICTA76 / 99754

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.