MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Avient Dynalloy™ OBC8000-T05 Thermoplastic Elastomer (TPE)
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Dynalloy™ OBC8000-T05 is an ultra-soft TPE utilizing the unique rubber properties of Dows INFUSE™ Olefin Block Copolymers. This product is designed for injection molding applications where exceptional softness and overmolding to polypropylene is desired New Product. Commercial specifications have not been established. - Adhesion to Polypropylene - Enhanced Flow - Excellent Colorability - Tactile Feel - Ultra Soft

Color concentrates with Dynalloy™ OBC8000-T05 as the carrier are most suitable for coloring this product. If a OBC8000-T05 color concentrate carrier is desired, it is important that the chosen color house have underwater pelletization capabilities. Typical loadings for color concentrates are 1% to 5% by weight. Liquid color (pigment, not dye) can be used; white oil carriers are recommended. A high color match consistency can be obtained by using precolored compounds available from GLS. Polypropylene (PP) based color concentrates are not recommended because they lead to poor dispersion and can significantly change the hardness of the material. Concentrates based on PVC should not be used. The final determination of color concentrate suitability should be determined by customer trials. Purge thoroughly before and after use of this product with a low flow (0.5 - 2.5 MFR) polystyrene (PS) or polypropylene (PP). Regrind levels up to 20% can be used with Dynalloy™ OBC8000-T05 with minimal property loss, provided that the regrind is free of contamination. To minimize losses during molding, the melt tempetature should remain as low as possible. The final determination of regrind effectiveness should be determined by the customer. Dynalloy™ OBC8000-T05 has good melt stability. Maximum residence times may vary, depending on the size of the barrel. Generally, the barrel should be emptied if it is idle for periods of 8 - 10 minutes or longer. Drying is not Required Injection Speed: 0.5 to 3 in/sec 1st Stage - Boost Pressure: 200 to 700 psi 2nd Stage - Hold Pressure: 20% of Boost Hold Time (Thick Part): 1 to 5 sec Hold Time (Thin Part): 1 to 3 sec

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.868 g/cc0.868 g/ccASTM D792
Viscosity  7600 cP
@Shear Rate 11200 1/s,
Temperature 200 °C
7600 cP
@Shear Rate 11200 1/s,
Temperature 392 °F
ASTM D3835
 40000 cP
@Shear Rate 1340 1/s,
Temperature 200 °C
40000 cP
@Shear Rate 1340 1/s,
Temperature 392 °F
ASTM D3835
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore OO 575710 sec; ASTM D2240
Tensile Strength at Break 1.25 MPa
@Temperature 23.0 °C
181 psi
@Temperature 73.4 °F
Die C2 hr; ASTM D412
Tensile Stress at Strain  0.103 MPa
@Strain 100 %,
Temperature 23.0 °C
14.9 psi
@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
 0.207 MPa
@Strain 300 %,
Temperature 23.0 °C
30.0 psi
@Strain 300 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
Elongation at Break 1400 %
@Temperature 23.0 °C
1400 %
@Temperature 73.4 °F
Die C2 hr; ASTM D412
Compression Set  10 %
@Temperature 23.0 °C,
Time 79200 sec
10 %
@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395B
 19 %
@Temperature 40.0 °C,
Time 79200 sec
19 %
@Temperature 104 °F,
Time 22.0 hour
ASTM D395B
 35 %
@Temperature 70.0 °C,
Time 79200 sec
35 %
@Temperature 158 °F,
Time 22.0 hour
ASTM D395B
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 149 - 171 °C300 - 340 °F
Middle Barrel Temperature 166 - 188 °C331 - 370 °F
Front Barrel Temperature 177 - 199 °C351 - 390 °F
Nozzle Temperature 182 - 216 °C360 - 421 °F
Melt Temperature 182 - 216 °C360 - 421 °F
Mold Temperature 15.6 - 32.2 °C60.1 - 90.0 °F
Back Pressure 0.000 - 0.552 MPa0.000 - 80.1 psi
Screw Speed 80 - 120 rpm80 - 120 rpm
 
Compliance PropertiesMetricEnglishComments
FDA YesYes21 CFR 177.1210
 
Descriptive Properties
AppearanceTranslucent
FeaturesGood Colorability
 Good Flow
 Good Processing Stability
 Low Hardness
 Soft
FormsPellets
Generic MaterialTPE
Generic NameThermoplastic Elastomer (TPE)
Processing MethodInjection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
RoHS ComplianceRoHS Compliant
Suggested Max Regrind20%
UsesConsumer Applications
 Flexible Grips
 Overmolding
 Personal Care
 Seals
 Transparent or Translucent Parts

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Geon® Performance Solutions 130 Series 136 Polyvinyl Chloride Copolymer (PVC Copolymer)
Formosa Plastics Formolon® 113 PVC
Geon® Performance Solutions 130 Series 137 Polyvinyl Chloride Copolymer (PVC Copolymer)
Geon® Performance Solutions 130 Series 138 Polyvinyl Chloride Copolymer (PVC Copolymer)
Inovyn 460SL Polyvinyl Chloride grafted copolymer

PH0POL1168 / 145737

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.