MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Free-Cutting Brass, UNS C36000, H01 (Cold Drawn 15%) Temper shapes
Categories: Metal; Nonferrous Metal; Copper Alloy; Brass

Material Notes: Fair to excellent corrosion resistance. Excellent machinability. Fabricated by machining, roll threading and knurling.

Applications: gears, pinions, automatic high-speed screw machine parts.

Test specimen: shapes.

Key Words: free cutting, FC, CDA 360, CZ124, ISO CuZn36Pb3, CEN CW603N, FED QQ-B-626 (discontinued), ASTM-B121, ASTM-B36, ASTM-B16/B16M, ASTM-B124
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.50 g/cc0.307 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 6262
Tensile Strength, Ultimate 385 MPa55800 psi
Tensile Strength, Yield 310 MPa
@Strain 0.5 %
45000 psi
@Strain 0.5 %
Elongation at Break 20 %20 %In 50 mm
Modulus of Elasticity 97.0 GPa14100 ksi
Poissons Ratio 0.3110.311
Machinability 100 %100 %Excellent - the standard against which other copper alloys are judged
Shear Modulus 37.0 GPa5370 ksi
Shear Strength 230 MPa33400 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000660 ohm-cm
@Temperature 20.0 °C
0.00000660 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 20.5 µm/m-°C
@Temperature 20.0 - 300 °C
11.4 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.380 J/g-°C0.0908 BTU/lb-°F
Thermal Conductivity 115 W/m-K
@Temperature 20.0 °C
798 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point 885 - 900 °C1630 - 1650 °F
Solidus 885 °C1630 °F
Liquidus 900 °C1650 °F
Annealing Point 427 - 593 °C800 - 1100 °F
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 425 - 600 °C797 - 1110 °F
Hot-Working Temperature 700 - 800 °C1290 - 1470 °F
Recrystallization Temperature 330 °C626 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 60 - 63 %60 - 63 %
Iron, Fe <= 0.35 %<= 0.35 %
Lead, Pb 2.5 - 3.7 %2.5 - 3.7 %
Other, total <= 0.50 %<= 0.50 %
Zinc, Zn 35.5 %35.5 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Free-Cutting Brass, UNS C36000
Free-Cutting Brass, UNS C36000, H02 (Cold Drawn 25%) Temper 6 mm rod
Free-Cutting Brass, UNS C36000, Annealed Rod
Free-Cutting Brass, UNS C36000, H02 (Cold Drawn 20%) Temper 25 mm rod
Free-Cutting Brass, UNS C36000, H02 (Cold Drawn 18%) Temper 50 mm rod

MC36000b2 / 11239

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.