MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Eastman 9921P PET Injection Molded  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), Unreinforced

Material Notes: Voridian PET 9921P is produced at Voridian’s manufacturing sites in Rotterdam and Zarate, it is PTA/CHDM based, and it is sold to customers in the Europe, Middle East and Africa, Argentina, Bolivia, Brazil, Chile, Colombia, Mexico, Paraguay, Peru, Uruguay and Venezuela. Voridian PET 9921P will be used primarily for thick wall applications such as refill bottles for water and carbonated soft drinks.

Applications/Uses

  • APET and thick sheet
  • Beverage packaging
  • Custom containers
  • Thick wall containers
  • Bottles
  • Sealing layer for CPET trays
  • Refillable bottles
  • Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Specific Gravity 1.30 g/cc1.30 g/ccASTM D792
    Bulk Density 0.803 g/cc0.0290 lb/in³Poured; ASTM D1895
     0.881 g/cc0.0318 lb/in³Vibrated; ASTM D1895
    Density 1.30 g/cc0.0470 lb/in³ISO 1183
     1.40 g/cc0.0506 lb/in³Crystalline Density; ASTM D1505
    Melt Density 1.20 g/cc
    @Temperature 285 °C
    0.0434 lb/in³
    @Temperature 545 °F
    ASTM D1238
    Viscosity Measurement 0.78 - 0.820.78 - 0.82Pellet, Intrinsic; VGAS-A-AN-G-V-1
     
    Mechanical PropertiesMetricEnglishComments
    Hardness, Rockwell R 111111ASTM D785
    Tensile Strength at Break 26.0 MPa3770 psiISO 527
     31.0 MPa4500 psiASTM D638
    Tensile Strength, Yield 54.0 MPa7830 psiISO 527
     55.0 MPa7980 psiASTM D638
    Elongation at Break 114 %114 %ISO 527
     173 %173 %ASTM D638
    Tensile Modulus 2.30 GPa334 ksiASTM D638
     2.332 GPa338.2 ksiISO 527
    Flexural Yield Strength 76.0 MPa11000 psiASTM D790
    Flexural Modulus 2.40 GPa348 ksiASTM D790
    Izod Impact, Notched  0.340 J/cm
    @Temperature -40.0 °C
    0.637 ft-lb/in
    @Temperature -40.0 °F
    ASTM D256
     0.790 J/cm
    @Temperature 23.0 °C
    1.48 ft-lb/in
    @Temperature 73.4 °F
    ASTM D256
    Izod Impact, Unnotched NBNBASTM D4812
     NB
    @Temperature -30.0 °C
    NB
    @Temperature -22.0 °F
    ASTM D4812
    Izod Impact, Notched (ISO)  3.90 kJ/m²
    @Temperature -40.0 °C
    1.86 ft-lb/in²
    @Temperature -40.0 °F
    ISO 180
     6.80 kJ/m²
    @Temperature 23.0 °C
    3.24 ft-lb/in²
    @Temperature 73.4 °F
    ISO 180
    Puncture Energy  8.20 J
    @Thickness 2.70 mm,
    Temperature -40.0 °C
    6.05 ft-lb
    @Thickness 0.106 in,
    Temperature -40.0 °F
    max load; ASTM D3763
     31.0 J
    @Thickness 2.70 mm,
    Temperature 23.0 °C
    22.9 ft-lb
    @Thickness 0.106 in,
    Temperature 73.4 °F
    max load; ASTM D3763
     
    Thermal PropertiesMetricEnglishComments
    Heat of Fusion 61.0 J/g26.2 BTU/lbASTM E793
    Specific Heat Capacity 1.20 J/g-°C0.287 BTU/lb-°FASTM E1269
     1.40 J/g-°C
    @Temperature 80.0 °C
    0.335 BTU/lb-°F
    @Temperature 176 °F
    ASTM E1269
     1.60 J/g-°C
    @Temperature 100 °C
    0.382 BTU/lb-°F
    @Temperature 212 °F
    ASTM E1269
     2.00 J/g-°C
    @Temperature 200 °C
    0.478 BTU/lb-°F
    @Temperature 392 °F
    ASTM E1269
     2.10 J/g-°C
    @Temperature 280 °C
    0.502 BTU/lb-°F
    @Temperature 536 °F
    ASTM E1269
    Melting Point 239 °C462 °FCrystalline Peak; ASTM D3418
    Deflection Temperature at 0.46 MPa (66 psi) 69.0 °C156 °FISO 75
     69.0 °C156 °FASTM D648
    Deflection Temperature at 1.8 MPa (264 psi) 63.0 °C145 °FASTM D648
     64.0 °C147 °FISO 75
     
    Descriptive Properties
    Acetaldehyde<1ppmVKCA-A-AS-G-GC-0001
    Color, CIE a*-3.5 to -0.5VGAS-A-AN-G-RS-001
    Color, CIE b*-2.5 to 1.5VGAS-A-AN-G-RS-001
    Color, CIE L*78 minVGAS-A-AN-G-RS-001
    Fines, wt%, max0.05VGAS-A-AN-G-GA-1
    Pellet ShapeRectangular 2x2x3 mm

    **
    Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

    Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    Eastman 9921 PET Injection Molded
    Dow LIGHTER™ S93 Polyethylene Terephthalate (PET) Resin
    Dow LIGHTER™ S98 Polyethylene Terephthalate (PET) Resin
    Eastman 9921W PET Injection Molded
    Overview of materials for Polyethylene Terephthalate (PET), Unreinforced

    PE9137 / 35194

    Aluminum Castings

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.