MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Nickel Iron Alloy 52 Sealing Wire, UNS N14052
Categories: Metal; Nonferrous Metal; Nickel Alloy

Material Notes: Designed for use with a variety of soft glasses. It has an almost constant coefficient of thermal expansion up to about 565°C (1050°F). Specific uses are glass to metal sealing applications with soft glass and ceramics. When used for sealing purposes, this alloy is usually in the annealed condition because residual cold work distorts the coefficient of thermal expansion.

Information provided by Alloywire International.

Key Words: W.NR 2.4478; AWS 093
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.30 g/cc0.300 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 450 - 550 MPa65300 - 79800 psiAnnealed
 700 - 900 MPa102000 - 131000 psiHard Drawn
 
Thermal PropertiesMetricEnglishComments
CTE, linear 10.3 µm/m-°C
@Temperature 20.0 - 100 °C
5.72 µin/in-°F
@Temperature 68.0 - 212 °F
Thermal Conductivity 17.0 W/m-K118 BTU-in/hr-ft²-°F
Melting Point 1450 °C2640 °F
Maximum Service Temperature, Air 450 °C842 °Fannealed or hard drawn
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 850 - 1000 °C1560 - 1830 °Fusually used in annealed condition
 
Component Elements PropertiesMetricEnglishComments
Iron, Fe 48 %48 %as balance
Nickel, Ni 52 %52 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
California Fine Wire Alloy 52 Nickel Iron Alloy
Kanthal® 52 Nickel-Iron Resistor Alloy
Special Metals INCONEL® Alloy 601
304 Stainless Steel
High-Nickel Iron, heat-resistant gray iron

MN52 / 88082

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.