MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

ExxonMobil Santoprene® 281-64MED Thermoplastic Elastomer  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of our medical grades. Prior to release, each medical grade lot undergoes a Cytotoxicity study using the ISO elution method and a Physico-Chemical - Elastomeric Closures test for heavy metals such as lead. This grade of Santoprene TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It is polyolefin based and completely recyclable.

Information provided by Advanced Elastomer Systems

Key Words: EU 2003/11/EC; RoHS Compliant; USP Class VI
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.970 g/cc0.970 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6464.12 in; ASTM D2240
Tensile Strength at Break 6.420 MPa931.2 psiAir at 212°F, 168 hr; ASTM D573
 6.69 MPa970 psiAcross Flow; ASTM D412
Tensile Strength, Ultimate 2.48 MPa360 psiAcross Flow; ASTM D412
Elongation at Break 482.3 %482.3 %Air at 212°F, 168 hr; ASTM D573
 530 %530 %Across Flow; ASTM D412
Tear Strength 9.99 kN/m57.0 pli212°F, Die C; ASTM D624
 24.0 kN/m137 pli73°F, Die C; ASTM D624
Compression Set  22 %
@Temperature 22.8 °C,
Time 605000 sec
22 %
@Temperature 73.0 °F,
Time 168 hour
ASTM D395
 54 %
@Temperature 100 °C,
Time 605000 sec
54 %
@Temperature 212 °F,
Time 168 hour
ASTM D395
 
Processing PropertiesMetricEnglishComments
Processing Temperature 175 - 230 °C347 - 446 °F
 
Compliance PropertiesMetricEnglishComments
USP Class VI YesYes
 
Descriptive Properties
ColorNatural Color
FormPellets

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil Santoprene® 8281-65MED Thermoplastic Elastomer
ExxonMobil Santoprene® 8281-35MED Thermoplastic Elastomer
ExxonMobil Santoprene® 8281-55MED Thermoplastic Elastomer
Advanced Elastomer Systems Santoprene® 181-55 Thermoplastic Rubber
ExxonMobil Santoprene® 8281-45MED Thermoplastic Elastomer

PADVA137 / 22827

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.