MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AISI Type S24100 Stainless Steel 6.4 mm diameter annealed rod, 30% cold reduction
Categories: Metal; Ferrous Metal; Heat Resisting; Stainless Steel; T S20000 Series Stainless Steel

Material Notes: Low nickel, austenitic with comparable corrosion resistance, high work hardenability permits cold drawing to high-strength levels while maintaining good ductility, excellent wear- and galling-resistance, resists staining and rusting in 5% sodium chloride fog and high-humidity atmospheres, readily welded. Applications include high-strength shafting and bolting, clamps for pole line hardware, concrete reinforcing accessories, abrasion and corrosion resistant screens, high-strength nonmagnetic springs, wire forms, racks and cages.

Key Words: UNS S24100, ASTM A276 (XM-28), ASTM A313 (XM-28), ASTM A580 (XM-28)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.78 g/cc0.281 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 305305Converted from Rockwell C hardness.
Hardness, Knoop 326326Converted from Rockwell C hardness.
Hardness, Rockwell C 3232
Hardness, Vickers 316316Converted from Rockwell C hardness.
Tensile Strength, Ultimate 1310 MPa190000 psi
Tensile Strength, Yield 1090 MPa
@Strain 0.2 %
158000 psi
@Strain 0.2 %
Elongation at Break 18.5 %18.5 %Gage length is 4 times specimen diameter or in 50 mm.
Modulus of Elasticity 200 GPa29000 ksiTypical for stainless steel
Machinability 30 %30 %Based on 100% machinability for AISI 1212 steel.
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000660 ohm-cm0.0000660 ohm-cmTypical value for stainless steel.
Magnetic Permeability 1.008 - 1.0111.008 - 1.011H = 200 Oe. Value = 1.008 annealed. Value = 1.011 when 70% cold drawn.
 
Thermal PropertiesMetricEnglishComments
CTE, linear  16.2 µm/m-°C
@Temperature 24.0 - 95.0 °C
9.00 µin/in-°F
@Temperature 75.2 - 203 °F
 16.9 µm/m-°C
@Temperature 24.0 - 205 °C
9.39 µin/in-°F
@Temperature 75.2 - 401 °F
 17.6 µm/m-°C
@Temperature 24.0 - 315 °C
9.78 µin/in-°F
@Temperature 75.2 - 599 °F
 18.0 µm/m-°C
@Temperature 24.0 - 425 °C
10.0 µin/in-°F
@Temperature 75.2 - 797 °F
 18.5 µm/m-°C
@Temperature 24.0 - 540 °C
10.3 µin/in-°F
@Temperature 75.2 - 1000 °F
 19.3 µm/m-°C
@Temperature 24.0 - 650 °C
10.7 µin/in-°F
@Temperature 75.2 - 1200 °F
 19.8 µm/m-°C
@Temperature 24.0 - 760 °C
11.0 µin/in-°F
@Temperature 75.2 - 1400 °F
 20.2 µm/m-°C
@Temperature 24.0 - 870 °C
11.2 µin/in-°F
@Temperature 75.2 - 1600 °F
 20.9 µm/m-°C
@Temperature 24.0 - 980 °C
11.6 µin/in-°F
@Temperature 75.2 - 1800 °F
Specific Heat Capacity 0.480 J/g-°C0.115 BTU/lb-°FTypical value for stainless steel.
Thermal Conductivity 20.7 W/m-K144 BTU-in/hr-ft²-°FTypical value for stainless steel.
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.15 %<= 0.15 %
Chromium, Cr 18 %18 %
Iron, Fe 66 %66 %
Manganese, Mn 13 %13 %
Nickel, Ni 1.5 %1.5 %
Nitrogen, N 0.33 %0.33 %
Phosphorus, P <= 0.060 %<= 0.060 %
Silicon, Si <= 1.0 %<= 1.0 %
Sulfur, S <= 0.030 %<= 0.030 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI Type S24100 Stainless Steel 6.4 mm diameter annealed rod, 0% cold reduction
AISI Type S24100 Stainless Steel 6.4 mm diameter annealed rod, 10% cold reduction
AISI Type S20910 Stainless Steel, 6.4 mm diameter rod, annealed at 1120°C, 30% cold reduction
AISI Type S21800 Stainless Steel, 10% cold reduction
AISI Type S24100 Stainless Steel 6.4 mm diameter annealed rod, 60% cold reduction

MQM241M / 13801

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.