MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Petrothene® PR92735 Linear Low Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Extrusion Grade

Material Notes:

Applications
PETROTHENE PR 92735 is a high molecular weight, linear low density-based compound designed for cable jacketing. PR 92735 contains a nominal carbon black content of 2.6% and antioxidant has been added to ensure thermal stability during processing. PR 92735 also contains a processing aid.

Processing Techniques
PR 92735, like other thermoplastic polyolefin compounds, can be extruded as wire and cable insulation using a conventional extruder. However, it has been found that a high shear mixing screw design improves the processability of this type of material. A typical drawdown ratio for this material is 3.17:1. Below are suggested extrusion conditions for PR 92735. These conditions are intended as general guidelines only and are not optimum values, since manufacturing conditions, such as extruder type and size, affect the processing of thermoplastic compounds.

Industry Specifications
PR 92735 meets the requirements of the following: ASTM D 1248, Type 1, Category 4, Class C, Grades E5, J1 and J3 Federal LP 390C, Type 111, Class L, Grades 2, 3, and 4, Category 4: REA PE 200, Appendix E.

This product is from the former Equistar product line.

Key Words: LLDPE; Linear Low Density Polyethylene Black Jacket; Telecom/ Telecommunications; Jacketing
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.930 g/cc0.0336 lb/in³ASTM D1505
ESCR 10% Igepal® >= 1000 hour>= 1000 hourASTM D1693
Absorption Coefficient 440440ASTM D3349
Carbon Black Loading 2.6 %2.6 %
Melt Flow 0.59 g/10 min0.59 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5757ASTM D224
Tensile Strength at Break 16.5 MPa2400 psiASTM D638
Tensile Strength, Yield 11.0 MPa1600 psiASTM D638
Elongation at Break 650 %650 %ASTM D638
Flexural Modulus, 1% Secant 248 MPa36000 psiASTM D790
 365 MPa53000 psiASTM D790
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 2.5
@Frequency 1e+6 Hz
2.5
@Frequency 1e+6 Hz
ASTM D1531
Dielectric Strength 19.7 kV/mm500 kV/inASTM D149
Dissipation Factor 0.00040
@Frequency 1e+6 Hz
0.00040
@Frequency 1e+6 Hz
ASTM D1531
 
Thermal PropertiesMetricEnglishComments
CTE, linear 200 µm/m-°C
@Temperature 20.0 °C
111 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Brittleness Temperature <= -76.0 °C<= -105 °FF50; ASTM D746
 
Processing PropertiesMetricEnglishComments
Feed Temperature 154 - 163 °C310 - 325 °F
Zone 2 177 - 193 °C350 - 380 °F
Zone 3 193 - 210 °C380 - 410 °F
Zone 4-x 204 - 218 °C400 - 425 °F
Adapter Temperature 204 - 218 °C400 - 425 °F
Die Temperature 204 - 218 °C400 - 425 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Procom® D 1189 Polypropylene
LyondellBasell Petrothene® GA818073 Linear Low Density Polyethylene
BASF Procom® D 1188 Polypropylene
BASF Procom® D 1118 Polypropylene
NOVA Chemicals Novapol® PP-0118-F LLDPE Extrusion Resin

PEQU0288 / 36722

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.