MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Envalior Arnitel® EB464 TPC-ET, Blow Molding Grade
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyester TPE; Polyester, TP

Material Notes: Blow Molding Grade

Former DSM Engineering Plastics product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.15 g/cc0.0415 lb/in³ISO 1183
Water Absorption 0.70 %0.70 %Sim. ISO 62
Moisture Absorption 0.300 %0.300 %Humidity; Sim. ISO 62
Melt Flow 8.0 g/10 min
@Load 10.0 kg,
Temperature 230 °C
8.0 g/10 min
@Load 22.0 lb,
Temperature 446 °F
MVR, [cm3/10min]; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D  39
@Time 3.00 sec
39
@Time 0.000833 hour
ISO 868
 39
@Time 15.0 sec
39
@Time 0.00417 hour
ISO 868
Tensile Strength at Break 21.5 MPa3120 psiISO 527-1/-2
Tensile Stress at Strain  3.40 MPa
@Strain 5.0 %
493 psi
@Strain 5.0 %
ISO 527-1/-2
 4.00 MPa
@Strain 5.0 %
580 psi
@Strain 5.0 %
normal; ISO 527-1/-2
 6.00 MPa
@Strain 10 %
870 psi
@Strain 10 %
ISO 527-1/-2
 6.20 MPa
@Strain 10 %
899 psi
@Strain 10 %
normal; ISO 527-1/-2
 8.20 MPa
@Strain 50 %
1190 psi
@Strain 50 %
normal; ISO 527-1/-2
 10.5 MPa
@Strain 100 %
1520 psi
@Strain 100 %
normal; ISO 527-1/-2
 11.0 MPa
@Strain 50 %
1600 psi
@Strain 50 %
ISO 527-1/-2
 13.9 MPa
@Strain 100 %
2020 psi
@Strain 100 %
ISO 527-1/-2
 1.80 MPa
@Strain 10 %,
Temperature 100 °C
261 psi
@Strain 10 %,
Temperature 212 °F
parallel; ISO 527-1/-2
 5.00 MPa
@Strain 10 %,
Temperature 23.0 °C
725 psi
@Strain 10 %,
Temperature 73.4 °F
parallel; ISO 527-1/-2
 12.5 MPa
@Strain 10 %,
Temperature -40.0 °C
1810 psi
@Strain 10 %,
Temperature -40.0 °F
parallel; ISO 527-1/-2
Film Elongation at Break, MD 530 %530 %ISO 527-1/-2
Elongation at Break 300 %300 %Nominal; ISO 527-1/-2
Tensile Modulus 0.0670 GPa9.72 ksiISO 527-1/-2
Izod Impact, Notched (ISO)  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 180/1A
 NB
@Temperature -20.0 °C
NB
@Temperature -4.00 °F
ISO 180/1A
Charpy Impact, Notched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eA
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eA
Tear Strength Test 100100parallel, Graves (without nick); ISO 34
 110110normal, Graves (without nick); ISO 34
Film Tensile Strength at Break, MD 20.4 MPa2960 psiISO 527-1/-2
 
Thermal PropertiesMetricEnglishComments
Melting Point 213 °C415 °F10°C/min; ISO 11357-1/-3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Envalior Arnitel® EB463 TPC-ET, Blow Molding Grade
Celanese SO.F.TER Pibiflex® B 5050 MWR NERO Copolyester TPE
Envalior Arnitel® EB464-01 TPC-ET, Blow Molding Grade
Envalior Arnitel® PB420-B TPC-ET
Celanese Hytrel® HTR8223 BK320 TPC-ET

PDSM8103 / 184804

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.