MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for PVC, Foam Grade
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Foam Grade

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "PVC, Foam Grade". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 0.0400 - 1.50 g/cc0.00145 - 0.0542 lb/in³Average value: 0.559 g/cc Grade Count:84
Water Absorption 0.0300 - 4.00 %0.0300 - 4.00 %Average value: 1.22 % Grade Count:27
Water Vapor Transmission 0.900 - 7.50 g/m²/day0.0580 - 0.483 g/100 in²/dayAverage value: 4.14 g/m²/day Grade Count:8
Viscosity Number 110 - 200 cm³/g1.10 - 2.00 dl/gAverage value: 128 cm³/g Grade Count:8
Thickness 6350 - 69900 microns250 - 2750 milAverage value: 37300 microns Grade Count:4
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 42.0 - 96.042.0 - 96.0Average value: 59.9 Grade Count:23
Hardness, Shore D 47.0 - 85.047.0 - 85.0Average value: 68.7 Grade Count:15
Hardness, Shore OO 13.0 - 45.013.0 - 45.0Average value: 28.7 Grade Count:3
Tensile Strength, Ultimate 0.710 - 39.2 MPa103 - 5690 psiAverage value: 8.25 MPa Grade Count:50
Tensile Strength, Yield 0.103 - 51.6 MPa15.0 - 7480 psiAverage value: 18.8 MPa Grade Count:20
Elongation at Break 1.40 - 450 %1.40 - 450 %Average value: 127 % Grade Count:53
Modulus of Elasticity 0.0270 - 3.38 GPa3.92 - 490 ksiAverage value: 0.782 GPa Grade Count:51
Flexural Yield Strength 12.4 - 170 MPa1800 - 24700 psiAverage value: 50.0 MPa Grade Count:19
Flexural Modulus 0.994 - 3.79 GPa144 - 550 ksiAverage value: 1.86 GPa Grade Count:18
Compressive Yield Strength 0.00758 - 6.79 MPa1.10 - 985 psiAverage value: 1.97 MPa Grade Count:34
Compressive Modulus 0.0000138 - 0.600 GPa0.00200 - 87.0 ksiAverage value: 0.117 GPa Grade Count:35
Poissons Ratio 0.3200.320Average value: 0.320 Grade Count:8
Shear Modulus 0.0120 - 0.115 GPa1.74 - 16.7 ksiAverage value: 0.0376 GPa Grade Count:30
Shear Strength 0.460 - 5.01 MPa66.7 - 727 psiAverage value: 1.70 MPa Grade Count:30
Izod Impact, Notched 0.210 - 0.961 J/cm0.393 - 1.80 ft-lb/inAverage value: 0.401 J/cm Grade Count:17
Tensile Impact Strength 12.8 kJ/m²6.10 ft-lb/in²Average value: 12.8 kJ/m² Grade Count:3
Dart Drop Total Energy 5.34 - 178 J/cm0.0100 - 0.333 ft-lb/milAverage value: 20.7 J/cm Grade Count:10
Compression Set 3.20 - 8.00 %3.20 - 8.00 %Average value: 5.08 % Grade Count:5
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 1.00e+13 - 5.00e+14 ohm1.00e+13 - 5.00e+14 ohmAverage value: 1.73e+14 ohm Grade Count:3
 
Thermal PropertiesMetricEnglishComments
CTE, linear 30.0 - 104 µm/m-°C16.7 - 58.0 µin/in-°FAverage value: 56.4 µm/m-°C Grade Count:31
Specific Heat Capacity 1.13 - 1.90 J/g-°C0.270 - 0.454 BTU/lb-°FAverage value: 1.57 J/g-°C Grade Count:8
Thermal Conductivity 0.00209 - 0.125 W/m-K0.0145 - 0.870 BTU-in/hr-ft²-°FAverage value: 0.0394 W/m-K Grade Count:27
 0.0230 - 0.0420 W/m-K
@Temperature 10.0 - 10.0 °C
0.160 - 0.291 BTU-in/hr-ft²-°F
@Temperature 50.0 - 50.0 °F
Average value: 0.0311 W/m-K Grade Count:8
Insulation R Value 1.80 - 12.61.80 - 12.6Average value: 5.68 Grade Count:8
Maximum Service Temperature, Air 60.0 - 90.0 °C140 - 194 °FAverage value: 72.4 °C Grade Count:16
Deflection Temperature at 1.8 MPa (264 psi) 56.1 - 72.8 °C133 - 163 °FAverage value: 64.9 °C Grade Count:14
Vicat Softening Point 63.0 - 75.0 °C145 - 167 °FAverage value: 70.6 °C Grade Count:5
Minimum Service Temperature, Air -200 - 0.000 °C-328 - 32.0 °FAverage value: -110 °C Grade Count:16
 
Processing PropertiesMetricEnglishComments
Processing Temperature 80.0 - 129 °C176 - 264 °FAverage value: 86.9 °C Grade Count:9
Die Temperature 185 °C365 °FAverage value: 185 °C Grade Count:3
Melt Temperature 166 - 199 °C330 - 390 °FAverage value: 178 °C Grade Count:15

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for PVC, Molded
Overview of materials for PVC, Flexible Grade
Overview of materials for PVC, Extruded
Overview of materials for PVC, Sheet Grade
Overview of materials for PVC, High Impact

O5604 / 78515

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.