MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Arsenical Lead Cable-Sheathing Alloy, UNS L50310, Pipe, Extruded at 450°C (840°F), Water Quenched
Categories: Metal; Nonferrous Metal; Lead Alloy

Key Words: Lead Alloys
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 11.34 g/cc0.4097 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 77
Tensile Strength, Ultimate 22.0 MPa3190 psi
Elongation at Break 35 %35 %in 50 mm
Modulus of Elasticity 14.0 GPa2030 ksiPure Lead
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 24.0 J/g10.3 BTU/lb
CTE, linear 29.1 µm/m-°C
@Temperature 20.0 - 100 °C
16.2 µin/in-°F
@Temperature 68.0 - 212 °F
Pure Lead
Specific Heat Capacity 0.129 J/g-°C0.0308 BTU/lb-°F
Thermal Conductivity 33.0 W/m-K229 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Arsenic, As 0.15 %0.15 %
Bismuth, Bi 0.10 %0.10 %
Lead, Pb 99.6 %99.6 %
Tin, Sn 0.10 %0.10 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ASTM A570 Steel, grade A, sheet and strip
ASTM A570 Steel, grade 50
ASTM A570 Steel, grade 45
ASTM A570 Steel, grade 40
ASTM A570 Steel, grade 36

MLPb30 / 12222

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.