MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

ALIMEX ACP 5080R Aluminum Cast Material
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 5000 Series Aluminum Alloy; Aluminum Casting Alloy

Material Notes: Sizes range availability along with good mechanical and physical properties of ACP 5080R provide the Mold Tool Industry tooling materials solutions for the most challenging applications.

Information provided by ALIMEX GmbH

Homogenized and stress relieved

Key Words: AA 5083 (AlMg4.5Mn0.7) according to DIN EN 573-3
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.66 g/cc0.0960 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 7070
Tensile Strength, Ultimate 290 MPa42100 psiRm
Tensile Strength, Yield 130 MPa
@Strain 0.2 %
18900 psi
@Strain 0.2 %
Elongation at Break 16 %16 %
Modulus of Elasticity 70.0 GPa10200 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.000004914 ohm-cm0.000004914 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 24.3 µm/m-°C
@Temperature 20.0 °C
13.5 µin/in-°F
@Temperature 68.0 °F
Thermal Conductivity 109 - 140 W/m-K756 - 972 BTU-in/hr-ft²-°F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ALIMEX ACP 5080 Aluminum Cast Plate
Aluminum 5154-O
AISI 4140 Steel, annealed at 815°C (1500°F) furnace cooled 11°C (20°F)/hour to 665°C (1230°F), air cooled, 25 mm (1 in.) round
Alclad Aluminum 6061-T6, T651
Aluminum 5154-H112

NALIMEX01 / 14756

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.