MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Multibase Multi-Pro® 4008 RC Medium Impact 40% Glass Filled Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 40% Glass Fiber Filler

Material Notes: Multi-Pro 4008 RC is a chemically coupled glass reinforced polypropylene compound exhibiting highest flexural modulus, flex strength and high impact resistance. Heat resistance is high due to highly coupled glass fiber matrix.

Data provided by Multibase.

Key Words: PP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.22 g/cc0.0441 lb/in³ASTM D792-91
Linear Mold Shrinkage 0.0020 cm/cm0.0020 in/inASTM D955-89
Melt Flow 8.5 g/10 min8.5 g/10 min(Condition L) ASTM D-1238-94a
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 858510 sec; ASTM D-2240-95
Tensile Strength, Ultimate 70.3 MPa10200 psiASTM D638-95
Flexural Strength 113.3 MPa16430 psiASTM D790-95
Flexural Modulus 6.345 GPa920.3 ksiMethod 1, Proc. B; ASTM D-790-95
Izod Impact, Notched 0.800 J/cm1.50 ft-lb/inASTM D256-93a
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 163 °C325 °FASTM D648-95
Deflection Temperature at 1.8 MPa (264 psi) 146 °C295 °FASTM D648-95

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Entec Hypro™ F PPH-GF40 Natural Homopolymer Polypropylene, 40% Glass Reinforced
A. Schulman Gapex® RPP30DA10BK 30% Fiberglass Reinforced, Heat Stabilized, Homopolymer Polypropylene
Ravago Manufacturing Americas Echo® RPC40G BK Polypropylene Homopolymer
Multibase Multi-Pro® 4003 R Medium Impact 40% Glass Filled Polypropylene
Overview of materials for Polypropylene with 40% Glass Fiber Filler

PLA284 / 49681

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.