MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BYK Laponite® LV Clay Additive
Categories: Ceramic; Clay; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Laponite LV has been specially developed for use in high performance water based surface coatings to produce shear sensitive and thixotropic structure. It is particularly useful in formulations that contain high levels of emulsion resins and so have relatively low levels of free water available in which to disperse a rheological additive. These include:
  • automotive basecoats
  • industrial and protective coatings
  • wood coatings
When hydrated in deionised water at up to 3% concentration, Laponite LV will produce a clear and colourless colloidal dispersion of very low viscosity level, typically <50 mPas. The low viscosity of this dispersion makes it easy to produce a homogenous mixture when it is combined into a resin system. On addition to a wide range of types of emulsion resins, Laponite LV will produce an instantaneous build in viscosity of the system.

Information provided by Southern Clay Products

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 1.00 g/cc0.0361 lb/in³
Particle Mesh Size >= 250 Mesh>= 250 Mesh<2%
pH 9.89.82% suspension
Specific Surface Area 370 m²/g370 m²/g
 
Processing PropertiesMetricEnglishComments
Gel Time 22.0 min22.0 ming
 
Component Elements PropertiesMetricEnglishComments
H2O, Water <= 10 %<= 10 %Free
Loss on Ignition(%) 8.2 %8.2 %
MgO 27.5 %27.5 %
Na2O 2.8 %2.8 %
SiO2 59.5 %59.5 %
 
Descriptive Properties
Color/FormFree flowing white powder
Composition0.008Li2O

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BYK Laponite® SL25 Thickener
BYK Laponite® S485 Magnesium Aluminum Silicate
BYK Laponite® S482 Thickener
BYK Laponite® S Synthetic Layered Fluorosilicate
BYK Laponite® RDS Synthetic Layered Silicate

PBYK064 / 185061

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.