MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lanxess X_Butyl™ I4565P Butyl Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: LANXESS X_Butyl™ I4565P is a new butyl polymer that possesses ionic groups on the polymer backbone. The ionic interactions produce large changes in physical, mechanical and rheological properties including improved green strength, thermoplastic elastomer behavior and superior adhesive properties compared to traditional butyl rubber. In addition, LANXESS X_Butyl™ I4565P is available in pellet form, allowing for ease of incorporation. It is recommended to use LANXESS X_Butyl™ I4565P as a compound modifier.

Key In addition to the key properties of butyl rubber such as impermeability, LANXESS X_Butyl™ I4565P has:

  • increased green strength
  • improved adhesion
  • enhanced crack growth resistance
  • improved polymer filler interactions
  • higher damping characteristics
  • greater tear strength
  • thermoplastic elastomer-like properties
  • resists bacteria, mold and algae growth
Benefits:
  • pellet form allows for ease of incorporation and faster throughput, particularly for adhesive and TPE applications
  • enhanced crack growth resistance may result in longer lasting product
  • increased polarity results in LANXESS X_Butyl™ I4565P being easily blended with common elastomers
Applications:
  • Used as a compound modifier for the following:
  • inner liner
  • power transmission belts
  • asphalt modification
  • adhesives & sealants
  • hoses
  • curing bladders
  • plastics modifier
  • NVH

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.930 g/cc0.0336 lb/in³
Mooney Viscosity 52 - 60
@Temperature 125 °C
52 - 60
@Temperature 257 °F
(1+8)
 
Component Elements PropertiesMetricEnglishComments
Bromine, Br 0.300 - 0.700 %0.300 - 0.700 %(mol%)
 
Descriptive Properties
Content0.3-.0.5 mol%Ionic
 0.5-0.7 mol%Unsaturation

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Butyl Rubber (IIR, CIIR, BIIR)
Precision Polymer Engineering J70M Butyl Rubber
Trelleborg T528 Butyl Rubber
Sibur BK-1675N Butyl Rubber (IIR)
Trelleborg T620 Butyl Rubber

PLANY8647 / 209040

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.