MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Haynes Hastelloy® D-205 Corrosion Resistant Alloy  (discontinued **)
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: High silicon alloy based on the Ni-20Cr system. Its chief advantages over high silicon-iron based alloys are excellent formability, good resistance to elevated temperature embrittlement, and superior performance In many concentrations of sulfuric acid. D-205 alloy also possesses high resistance to stress corrosion cracking and is considerably more resistant to pitting corrosion than type 316L Stainless and Fe-17Cr-20Ni-5Si alloys.

Given these attributes, D-205 alloy constitutes an ideal sulfuric acid, plate-heat-exchanger material. Also the alloy is very useful for all hardware involved with the processing of highly oxidizing media. An added benefit is that the yield strength of D-205 can be more than doubled by age-hardening.

Information provided by Haynes.

Key Words: D205
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Environmental Stress Crack Resistance >= 1008 hour
@Temperature 154 °C
>= 1008 hour
@Temperature 309 °F
45% MgCl2
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 786 MPa114000 psiMill Annealed
 979 MPa142000 psiAged 24hrs/1000°F
Tensile Strength, Yield  338 MPa
@Strain 0.2 %
49000 psi
@Strain 0.2 %
Mill Annealed
 717 MPa
@Strain 0.2 %
104000 psi
@Strain 0.2 %
Aged 24hrs/1000°F
Elongation at Break 28.6 %28.6 %in 2in., Aged 24hrs/1000°F
 56.5 %56.5 %in 2in., Mill Annealed
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.030 %<= 0.030 %
Chromium, Cr 20 %20 %
Copper, Cu 2.0 %2.0 %
Iron, Fe 6.0 %6.0 %
Molybdenum, Mo 2.5 %2.5 %
Nickel, Ni 64.47 - 64.5 %64.47 - 64.5 %
Silicon, Si 5.0 %5.0 %
 
Descriptive Properties
Critical Pitting Temp30°C4% NaCl + 0.1% Fe2(SO4)3 + 0.01 M HCl

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ATI Allvac® Nickelvac® H-X Nickel Superalloy, Heat Treatment: 1177°C (2150°F) Anneal
Haynes Hastelloy® B-2 alloy, bright-annealed sheet, heat treated at 1149°C (2100°F), hydrogen cooled
Haynes Hastelloy® N, 1.6 mm sheet, heat treated at 1175°C, rapid air cooled
Haynes Hastelloy® B-3® alloy, 0% cold work
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 649°C (1200°F), aged 1000 hours

NHAD205 / 16786

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.