MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Wacker ELASTOSIL® LR 3066/30 A/B Liquid Silicone Rubber with Low Frictional Coefficient
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: Liquid silicone rubbers of the ELASTOSIL® LR 3066 series are paste-like, easily-pigmentable two-component compounds with short curing times and low coefficient of friction. In comparison with ELASTOSIL® LR 3003 grade the coefficient of friction is reduced by 50 -70%. Their vulcanizates are noted for their high transparency and excellent mechanical and electrical properties.

Properties: The products can be used within a temperature range of - 55 °C to + 210 °C. The addition of heat stabilizers at service temperatures of more than 180 °C is recommended.

Application: These grades are particularly suitable for the economical production of large series of injection-molded articles. Parts made from ELASTOSIL® LR 3066/30 A/B can be used for technical applications. These articles are also suitable for use in conjunction with foodstuffs. Provided appropriate processing, ELASTOSIL® LR 3066/30 A/B parts can be used for food contact applications in accordance with the Recommendation "XV. Silicones" of the BfR and FDA 21 CFR § 177.2600 under observance of any given limitations on extractable and volatile substances.

Information provided by Wacker.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 g/cc1.10 g/ccDIN EN ISO 1183-1 A
Viscosity  320000 cP
@Shear Rate 10.0 1/s
320000 cP
@Shear Rate 10.0 1/s
DIN 53019
 750000 cP
@Shear Rate 0.900 1/s
750000 cP
@Shear Rate 0.900 1/s
DIN 53019
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 3131DIN 53505
Tensile Strength 7.60 MPa1100 psiDIN 53504 S 1
Elongation at Break 620 %620 %DIN 53504 S 1
Tear Strength 32.1 kN/m183 pliASTM D 624 B
Compression Set 15 %
@Temperature 175 °C,
Time 79200 sec
15 %
@Temperature 347 °F,
Time 22.0 hour
after 6h/200°C post curing; DIN ISO 815-B
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 210 °C410 °Fheat stabilizers recommended > 180°C
Minimum Service Temperature, Air -55.0 °C-67.0 °F
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %Transparent, but not quantified
 
Processing PropertiesMetricEnglishComments
Cure Time 5.00 min
@Temperature 165 °C
0.0833 hour
@Temperature 329 °F
press cured, post cured 4 h/200 °C in ventilated air
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
AppearanceTransparent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Wacker ELASTOSIL® R 427/30 High Strength Silicone Base
Wacker ELASTOSIL® R plus 4105/40 Solid Silicone Rubber-Batch Grade
Wacker ELASTOSIL® LR 6262 A/B US Liquid Silicone Rubber
Wacker ELASTOSIL® LR 3002/35 A/B Low Viscous Liquid Rubber
Master Bond MasterSil 155 Silicone

PWACK9929 / 197528

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.