MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Envalior Akulon® K222-KGV4 /A PA6-GF20 FR(30)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 20% Glass Fiber Filled

Material Notes: 20% Glass Reinforced, Heat Stabilized, Flame Retardant (Halogen-phosphorous-free)

Former DSM Engineering Plastics product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.34 g/cc0.0484 lb/in³dry; ISO 1183
Water Absorption 6.5 %6.5 %Sim. To ISO 62
Moisture Absorption 2.00 %2.00 %Sim. To ISO 62
Linear Mold Shrinkage, Flow 0.0060 cm/cm0.0060 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.010 cm/cm0.010 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 45.0 MPa6530 psicond; ISO 527-1/-2
 80.0 MPa11600 psidry; ISO 527-1/-2
Elongation at Break 3.0 %3.0 %dry; ISO 527-1/-2
 15 %15 %cond; ISO 527-1/-2
Tensile Modulus 2.50 GPa363 ksicond; ISO 527-1/-2
 5.70 GPa827 ksidry; ISO 527-1/-2
Charpy Impact Unnotched  4.00 J/cm²
@Temperature -30.0 °C
19.0 ft-lb/in²
@Temperature -22.0 °F
cond; ISO 179/1eU
 4.00 J/cm²
@Temperature -30.0 °C
19.0 ft-lb/in²
@Temperature -22.0 °F
dry; ISO 179/1eU
 4.60 J/cm²
@Temperature 23.0 °C
21.9 ft-lb/in²
@Temperature 73.4 °F
dry; ISO 179/1eU
 9.30 J/cm²
@Temperature 23.0 °C
44.3 ft-lb/in²
@Temperature 73.4 °F
cond; ISO 179/1eU
Charpy Impact, Notched  0.400 J/cm²
@Temperature 23.0 °C
1.90 ft-lb/in²
@Temperature 73.4 °F
dry; ISO 179/1eA
 0.400 J/cm²
@Temperature -30.0 °C
1.90 ft-lb/in²
@Temperature -22.0 °F
dry; ISO 179/1eA
 0.400 J/cm²
@Temperature -30.0 °C
1.90 ft-lb/in²
@Temperature -22.0 °F
cond; ISO 179/1eA
 0.900 J/cm²
@Temperature 23.0 °C
4.28 ft-lb/in²
@Temperature 73.4 °F
cond; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmcond; IEC 60093
 1.00e+15 ohm-cm1.00e+15 ohm-cmdry; IEC 60093
Surface Resistance 1.00e+14 ohm1.00e+14 ohmcond; IEC 60093
Dielectric Constant  3.8
@Frequency 1e+6 Hz
3.8
@Frequency 1e+6 Hz
dry; IEC 60250
 3.9
@Frequency 1e+6 Hz
3.9
@Frequency 1e+6 Hz
cond; IEC 60250
 4.3
@Frequency 100 Hz
4.3
@Frequency 100 Hz
dry; IEC 60250
 10
@Frequency 100 Hz
10
@Frequency 100 Hz
cond; IEC 60250
Dielectric Strength 25.0 kV/mm635 kV/incond; IEC 60243-1
 30.0 kV/mm762 kV/indry; IEC 60243-1
Dissipation Factor  0.013
@Frequency 100 Hz
0.013
@Frequency 100 Hz
dry; IEC 60250
 0.021
@Frequency 1e+6 Hz
0.021
@Frequency 1e+6 Hz
dry; IEC 60250
 0.10
@Frequency 1e+6 Hz
0.10
@Frequency 1e+6 Hz
cond; IEC 60250
 0.30
@Frequency 100 Hz
0.30
@Frequency 100 Hz
cond; IEC 60250
Comparative Tracking Index 600 V600 Vcond; IEC 60112
 600 V600 Vdry; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °F10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 210 °C410 °Fdry; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 170 °C338 °Fdry; ISO 75-1/-2
Flammability, UL94  V-2
@Thickness 1.50 mm
V-2
@Thickness 0.0591 in
dry; IEC 60695-11-10
 V-2
@Thickness 0.800 mm
V-2
@Thickness 0.0315 in
dry; IEC 60695-11-10
Glow Wire Flammability Index  960 °C
@Thickness 1.60 mm
1760 °F
@Thickness 0.0630 in
Dry; IEC 60695-2-12
 960 °C
@Thickness 1.00 mm
1760 °F
@Thickness 0.0394 in
Dry; IEC 60695-2-12

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Envalior Akulon® K222-KGV4 PA6-GF20 FR(30), Dry, 20% Glass Filled, Heat Stabilized, Flame Retardant
Envalior Akulon® K222-KGV4 PA6-GF20 FR(30), Conditioned, 20% Glass Filled, Heat Stabilized, Flame Retardant
Envalior Durethan® DP 1801/30 H3.0 000000 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Flame Retardant, Conditioned
Envalior Arnite® AV2 365 SN PET-30% Glass Reinforced (European Grade)
Envalior Durethan® DP 1801/30 H3.0 000000 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Flame Retardant, Dry

PDSM9725 / 161346

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.