MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Beijing Evergrow Resources MC Nylon
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes:

Information provided by Beijing Evergrow Resources.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.15 g/cc0.0415 lb/in³GB1033
Water Absorption 6.3 - 6.5 %6.3 - 6.5 %
Moisture Absorption 1.8 - 2.0 %1.8 - 2.0 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 80 - 8580 - 85GB3398
Ball Indentation Hardness 164 MPa23800 psiGB3398
Tensile Strength at Break 89.0 MPa12900 psiGB/T 1040
Elongation at Yield 29 %29 %GB/T 1040
Flexural Strength 96.0 MPa13900 psiGB9341
Compressive Strength 85.0 - 100 MPa12300 - 14500 psiGB/T 1040
Izod Impact, Notched (ISO) 5.70 kJ/m²2.71 ft-lb/in²GBT1043
Coefficient of Friction 0.400.40GB3360
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmVolume; GB1410
Arc Resistance 600 sec600 secASTM D112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 75.0 µm/m-°C41.7 µin/in-°FGB1036
Melting Point 223 °C433 °FHG/T2235
Heat Distortion Temperature 125 °C257 °FGB1634

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Acetal Copolymer, Unreinforced
Overview of materials for Acrylic, Optical Sheet
CeramTec Rubalit® HSS Alumina, 75% (High Strength Substrate)
Mitsubishi Chemical Advanced Materials Nylatron™ MC™ 907 / Ertalon™ 6 PLA PA6 Unfilled Type 6 nylon
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced

PBEIJ107 / 90176

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.