MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

California Fine Wire Platinum- 8%Tungsten Alloy (Alloy 436)
Categories: Metal; Nonferrous Metal; Precious Metal; Platinum Alloy

Material Notes: All values may vary dependent on specific design and usage

Capabilities:

  • Wire
  • Ribbon
  • Insulated
  • Plated

Information provided by California Fine Wire.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 21.2 g/cc0.765 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 1030 MPa150000 psiAnnealed
 1290 MPa187000 psiStress relieved
 1380 MPa200000 psiHard
Modulus of Elasticity 138 GPa20000 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000665 ohm-cm0.0000665 ohm-cm3% tolerance on sizes below 0.02, 5% tolerance on sizes above 0.02
 
Thermal PropertiesMetricEnglishComments
Melting Point 1870 °C3398 °F
 
Component Elements PropertiesMetricEnglishComments
Platinum, Pt 92 %92 %
Tungsten, W 8.0 %8.0 %
 
Descriptive Properties
MagneticNone
Temperature Coefficient of Resistance0.00021 ohms/ohm-°C0-100°C
Thermal EMF vs. Copper+0.007 mV

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Pt-3.5% Rh Alloy, Annealed
Goodfellow Platinum 92/Tungsten 8 Alloy
Pt-8% W Alloy, Annealed
Pt-8% W Alloy, Hard
CMW® ELKONIUM 302 platinum based alloy

NCALZ15 / 15558

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.