MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AdvanSource Biomaterials HydroSlip™ C Hydrophilic Polyether Aliphatic Polyurethane
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyether Grade

Material Notes: AdvanSource Biomaterials Corporation manufactures and markets thermoplastic elastomeric hydrogels under the tradename HydroThane™. HydroThane™ is a generic family of polyurethane hydrogels, with each grade having its own specific water absorption characteristics.

HydroThane™ is a family of super absorbent thermoplastic, hydrophilic aliphatic polyurethane elastomers, ranging in water absorption from 5 to 25% by weight, and is offered as a clear resin in durometer hardnesses of 80A & 93 Shore A. The outstanding characteristics of this family of compounds are the ability to rapidly absorb water, high tensile strength and high elongation. The result is a polymer having lubricious characteristics, as well as being inherently bacterial resistant due to the exceptionally high water content at the surface.

HydroThane™ hydrophilic polyurethane resins are thermoplastic hydrogels, which can be extruded or molded, by conventional means. Traditional hydrogels on the other hand, are thermosetting in nature, often making them difficult to fabricate, assemble , and sterilize. In addition, HydroThane pellets are elastomeric even when dehydrated, thus requiring no special storage conditions.

Information provided by AdvanSource Biomaterials Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.15 - 1.17 g/cc0.0415 - 0.0423 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 80 - 9380 - 93
Coefficient of Friction 0.0110.011
 
Thermal PropertiesMetricEnglishComments
Softening Point 110 - 132 °C230 - 270 °F
 
Descriptive Properties
Linear Expansion1.8
Water Content0.95

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AdvanSource Biomaterials HydroMed™ D640 Permanently Lubricious Polyurethane Coating
ATI Allvac® Vasco® 316-L Specialty Steel, Heat Treatment: 1038°C (1900°F) Anneal
AdvanSource Biomaterials ChronoFlex® C 80A Biodurable Medical Grade Polyurethane
AdvanSource Biomaterials ChronoFlex® C 75D Biodurable Medical Grade Polyurethane
AdvanSource Biomaterials ChronoPrene™ 25A Thermoplastic Rubber Elastomer

PCARDI11 / 27935

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.