MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Copper, UNS C62300 (Aluminum Bronze 9%), Annealed Rod
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: Good to excellent corrosion resistance. Good hot and cold formability. Fabricated by bending, hot pressing, forming, and welding.

Applications: bearings, bushings, valve guides, gears, valve seats, nuts, bolts, pump rods, work gears, and cams.

Key Words: CDA 623, CA106, ISO CuAl8Fe3
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 7.65 g/cc0.276 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell  46
@Load 3000 kg,
Temperature 538 °C
46
@Load 6610 lb,
Temperature 1000 °F
 97
@Load 3000 kg,
Temperature 427 °C
97
@Load 6610 lb,
Temperature 801 °F
 146
@Load 3000 kg,
Temperature 316 °C
146
@Load 6610 lb,
Temperature 601 °F
 151
@Load 3000 kg,
Temperature 204 °C
151
@Load 6610 lb,
Temperature 399 °F
 161
@Load 3000 kg,
Temperature 20.0 °C
161
@Load 6610 lb,
Temperature 68.0 °F
 168
@Load 3000 kg,
Temperature -29.0 °C
168
@Load 6610 lb,
Temperature -20.2 °F
 171
@Load 3000 kg,
Temperature -60.0 °C
171
@Load 6610 lb,
Temperature -76.0 °F
 195
@Load 3000 kg,
Temperature -182 °C
195
@Load 6610 lb,
Temperature -296 °F
Tensile Strength, Ultimate  94.0 MPa
@Temperature 538 °C
13600 psi
@Temperature 1000 °F
 210 MPa
@Temperature 427 °C
30500 psi
@Temperature 801 °F
 448 MPa
@Temperature 316 °C
65000 psi
@Temperature 601 °F
 534 MPa
@Temperature 204 °C
77500 psi
@Temperature 399 °F
 620 MPa
@Temperature 20.0 °C
89900 psi
@Temperature 68.0 °F
 647 MPa
@Temperature -29.0 °C
93800 psi
@Temperature -20.2 °F
 664 MPa
@Temperature -60.0 °C
96300 psi
@Temperature -76.0 °F
 762 MPa
@Temperature -182 °C
111000 psi
@Temperature -296 °F
Tensile Strength, Yield  84.0 MPa
@Strain 0.5 %,
Temperature 538 °C
12200 psi
@Strain 0.5 %,
Temperature 1000 °F
 153 MPa
@Strain 0.5 %,
Temperature 427 °C
22200 psi
@Strain 0.5 %,
Temperature 801 °F
 288 MPa
@Strain 0.5 %,
Temperature 316 °C
41800 psi
@Strain 0.5 %,
Temperature 601 °F
 294 MPa
@Strain 0.5 %,
Temperature 20.0 °C
42600 psi
@Strain 0.5 %,
Temperature 68.0 °F
 302 MPa
@Strain 0.5 %,
Temperature 204 °C
43800 psi
@Strain 0.5 %,
Temperature 399 °F
 323 MPa
@Strain 0.5 %,
Temperature -29.0 °C
46800 psi
@Strain 0.5 %,
Temperature -20.2 °F
 330 MPa
@Strain 0.5 %,
Temperature -60.0 °C
47900 psi
@Strain 0.5 %,
Temperature -76.0 °F
 377 MPa
@Strain 0.5 %,
Temperature -182 °C
54700 psi
@Strain 0.5 %,
Temperature -296 °F
Elongation at Break  10 %
@Temperature 316 °C
10 %
@Temperature 601 °F
 20 %
@Temperature 204 °C
20 %
@Temperature 399 °F
 27 %
@Temperature 538 °C
27 %
@Temperature 1000 °F
 31 %
@Temperature -29.0 °C
31 %
@Temperature -20.2 °F
 32 %
@Temperature 20.0 °C
32 %
@Temperature 68.0 °F
 33 %
@Temperature -60.0 °C
33 %
@Temperature -76.0 °F
 35 %
@Temperature -182 °C
35 %
@Temperature -296 °F
 46 %
@Temperature 427 °C
46 %
@Temperature 801 °F
Reduction of Area  13 %
@Temperature 316 °C
13 %
@Temperature 601 °F
 21 %
@Temperature 204 °C
21 %
@Temperature 399 °F
 32 %
@Temperature 538 °C
32 %
@Temperature 1000 °F
 38 %
@Temperature -29.0 °C
38 %
@Temperature -20.2 °F
 38 %
@Temperature -182 °C
38 %
@Temperature -296 °F
 39 %
@Temperature -60.0 °C
39 %
@Temperature -76.0 °F
 39 %
@Temperature 20.0 °C
39 %
@Temperature 68.0 °F
 39 %
@Temperature 427 °C
39 %
@Temperature 801 °F
Modulus of Elasticity 115 GPa16700 ksi
 51.0 GPa
@Temperature 538 °C
7400 ksi
@Temperature 1000 °F
 73.0 GPa
@Temperature 427 °C
10600 ksi
@Temperature 801 °F
 79.0 GPa
@Temperature 316 °C
11500 ksi
@Temperature 601 °F
 120 GPa
@Temperature 20.0 °C
17400 ksi
@Temperature 68.0 °F
 121 GPa
@Temperature -60.0 °C
17500 ksi
@Temperature -76.0 °F
 124 GPa
@Temperature -29.0 °C
18000 ksi
@Temperature -20.2 °F
 125 GPa
@Temperature -182 °C
18100 ksi
@Temperature -296 °F
 138 GPa
@Temperature 204 °C
20000 ksi
@Temperature 399 °F
Poissons Ratio 0.3280.328
Fatigue Strength 200 MPa
@# of Cycles 1.00e+8
29000 psi
@# of Cycles 1.00e+8
Reverse Bending
Machinability 50 %50 %
Forgeability 75 %75 %
Shear Modulus 44.0 GPa6380 ksi
Charpy Impact  9.00 J
@Temperature 427 °C
6.64 ft-lb
@Temperature 801 °F
V-notch
 10.0 J
@Temperature 538 °C
7.38 ft-lb
@Temperature 1000 °F
V-notch
 14.0 J
@Temperature -182 °C
10.3 ft-lb
@Temperature -296 °F
V-notch
 18.0 J
@Temperature -60.0 °C
13.3 ft-lb
@Temperature -76.0 °F
V-notch
 20.0 J
@Temperature -29.0 °C
14.8 ft-lb
@Temperature -20.2 °F
V-notch
 21.0 J
@Temperature 20.0 °C
15.5 ft-lb
@Temperature 68.0 °F
V-notch
 31.0 J
@Temperature 204 °C
22.9 ft-lb
@Temperature 399 °F
V-notch
 31.0 J
@Temperature 316 °C
22.9 ft-lb
@Temperature 601 °F
V-notch
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000144 ohm-cm
@Temperature 20.0 °C
0.0000144 ohm-cm
@Temperature 68.0 °F
Magnetic Permeability 1.171.17
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.2 µm/m-°C
@Temperature 20.0 - 300 °C
9.00 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.375 J/g-°C0.0896 BTU/lb-°F
Thermal Conductivity 54.4 W/m-K
@Temperature 20.0 °C
378 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point 1040 - 1045 °C1900 - 1913 °F
Solidus 1040 °C1900 °F
Liquidus 1045 °C1913 °F
Annealing Point 593 - 649 °C1100 - 1200 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 1010 °C1850 °FHot-Shortness Temperature
Annealing Temperature 600 - 650 °C1110 - 1200 °F
Hot-Working Temperature 700 - 875 °C1290 - 1610 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 8.5 - 11 %8.5 - 11 %
Copper, Cu 82.2 - 89.5 %82.2 - 89.5 %
Iron, Fe 2.0 - 4.0 %2.0 - 4.0 %
Manganese, Mn <= 0.50 %<= 0.50 %
Other, total <= 0.50 %<= 0.50 %
Silicon, Si <= 0.25 %<= 0.25 %
Tin, Sn <= 0.60 %<= 0.60 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Copper, UNS C62300 (Aluminum Bronze 9%), Cold Finished Rod
Copper, UNS C62300 (Aluminum Bronze 9%), H50 Temper 25-50 mm rod
AGC Fluon® PB3060 60% Bronze, PTFE Filled Compound
Aluminum Bronze, UNS C95410, Copper Casting Alloy, TQ50 Temper
ATI Allegheny Ludlum AL 276™ Nickel-Base Alloy, UNS N10276

MC62300c2 / 171646

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.