MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow Silastic® RBL-9200-20 LSR Liquid Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: SILASTIC™ RBL-9200 Series LSR elastomers and XIAMETER™ RBL-2004 Series LSR elastomers are general-purpose injection-molding materials suitable for a wide range of typical silicone rubber applications.

Product applications:

  • Consumer goods articles
  • Food contact applications

    Water approved applications

  • Infant care
  • Consumer electronics
  • Valves and diaphragms
  • Grommets, seals and gaskets
Key Features:
  • Unique rheology
  • Improved flowability
  • Longer pot life
  • Translucent
  • Food and water contact

Former Dow Corning brand.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 g/cc1.10 g/ccASTM D792
Viscosity  120000 cP
@Frequency 10 Hz
120000 cP
@Frequency 10 Hz
Part A; CTM 1094
 130000 cP
@Frequency 10 Hz
130000 cP
@Frequency 10 Hz
Part B; CTM 1094
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 1717ASTM D2240
Tensile Strength 6.20 MPa899 psiASTM D412
Elongation at Break 930 %930 %ASTM D412
Tear Strength 21.0 kN/m120 pliASTM D624 DIE B
Compression Set  18 %
@Temperature 175 °C,
Time 79200 sec
18 %
@Temperature 347 °F,
Time 22.0 hour
PC; 10 min @ 175°C + 4 hr @ 200°C; ASTM D395
 59 %
@Temperature 175 °C,
Time 79200 sec
59 %
@Temperature 347 °F,
Time 22.0 hour
NPC; 10 min @ 175°C; ASTM D395
 
Compliance PropertiesMetricEnglishComments
FDA YesYesFood Contact; FDA 21 CFR 177.2600

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow Silastic® FL 30-9201 F-LSR Fluoro Liquid Silicone Rubber
Dow XIAMETER™ RBL-2004-40 LSR Liquid Silicone Rubber
Momentive Performance Materials TUFEL™ II 94506 Low Volatile Extrusion Heat Cured Rubber
NuSil MED-4050 Silicone, Two Part High Consistency Elastomer - Restricted Medical Use
Dow Silastic® RBL-9200-30 LSR Liquid Silicone Rubber

PDOW9900 / 233103

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.