MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont™ Kevlar® Aramid Pulp
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoset; Aramid

Material Notes: Sold as highly fibrillated, short (0.5-1mm) fibers. Kevlar® pulps are chopped fibers that can be used as specialty additives to enhance performance by providing excellent reinforcement and viscosity control under shear stress. Kevlar® pulp is used in automotive brake pads, gaskets, automatic transmission papers, and as a viscosity control additive for adhesives and sealants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.45 g/cc1.45 g/cc
Bulk Density 0.0481 - 0.112 g/cc0.00174 - 0.00405 lb/in³
Specific Surface Area 7.0 - 11 m²/g7.0 - 11 m²/g
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 350 °C662 °F
Minimum Service Temperature, Air -200 °C-328 °F
 
Descriptive Properties
ColorYellow

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont™ Kevlar® 49 Aramid Fiber
DuPont™ Kevlar® 29 Aramid Fiber
DuPont™ Kevlar® 149 Aramid Fiber, diam. 12 µm
DuPont™ Nomex® 430 1600 Denier Aramid Yarn
Solvay Thornel® P-75 Carbon Fiber/Epoxy Advanced Composite System

PDUKEVP / 90028

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.