MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Spartech Royalite R570M Brominated ABS Resin  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant

Material Notes: Data provided by the manufacturer. The properties of this fire-rated ABS resin make it ideal for use in a variety of household products from electric weed trimmers and hedge trimmers to blenders, mixers and hair dryers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.28 g/cc0.0462 lb/in³ASTM D792
Water Absorption 0.030 %0.030 %24 hrs. ASTM D570
Viscosity 159300 cP
@Shear Rate 3000 1/s,
Temperature 191 °C
159300 cP
@Shear Rate 3000 1/s,
Temperature 375 °F
Melt Viscosity
Linear Mold Shrinkage 0.0060 cm/cm0.0060 in/inASTM D955
Melt Flow 1.1 g/10 min
@Load 5.00 kg,
Temperature 200 °C
1.1 g/10 min
@Load 11.0 lb,
Temperature 392 °F
Condition G; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 103103ASTM D785
Tensile Strength, Yield 50.1 MPa7270 psiASTM D638
Modulus of Elasticity 2.40 GPa348 ksiASTM D638
Flexural Yield Strength 81.4 MPa11800 psiASTM D790
Flexural Modulus 2.70 GPa392 ksiASTM D790
Izod Impact, Notched 3.30 J/cm6.18 ft-lb/inASTM D256
 0.900 J/cm
@Temperature -20.0 °C
1.69 ft-lb/in
@Temperature -4.00 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
CTE, linear 144 µm/m-°C
@Temperature 20.0 °C
80.0 µin/in-°F
@Temperature 68.0 °F
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 97.0 °C207 °FAnnealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 91.0 °C196 °FAnnealed; ASTM D648
Vicat Softening Point 93.0 °C199 °FASTM D1525
Flammability, UL94 5VA
@Thickness 3.20 mm
5VA
@Thickness 0.126 in
UL94
Oxygen Index 30.9 %30.9 %ASTM D2863

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Spartech Royalite R561M Low Smoke Resin
Huntsman IROGRAN® A 85 P 5004 TPU-Polyether
Calsak CS-72 General Purpose ABS Resin
Teknor Apex Elexar® EL 1934D Thermoplastic Elastomer
Spartech Royalite R722 PVC Alloy Aircraft Grade Sheet

ZPROY35 / 66395

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.