MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Syensqo (Solvay Specialty Polymers) Solef® 1006 Polyvinylidene Fluoride (PVDF)  (discontinued **)
Categories: Polymer; Thermoplastic; Fluoropolymer; Polyvinylidene Fluoride (PVDF); Polyvinylidinefluoride (PVDF), Molded/Extruded

Material Notes: Solef® 1006 PVDF is a very low viscosity homopolymer resin mainly used in injection molding or in multifilament extrusion.

Features: Homopolymer; Low Viscosity

Uses: General Purpose

Additional Properties: Charpy Notched Impact Strength - ASTM D6110 (23°C, 4.00 mm): 25.0 to 75.0 J/m; Coefficient of Friction - ASTM D1894 0.150 to 0.350; Coefficient of Friction - ASTM D1894 0.200 to 0.400; Crystallization Heat - ASTM D3417 54.0 to 60.0 J/g; Crystallization Point - ASTM D3418 137 to 144 °C; Heat of Fusion - ASTM D3417 58.0 to 67.0 J/g; Mold Shrinkage - 2.0 to 3.0 %

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.75 - 1.80 g/cc0.0632 - 0.0650 lb/in³ASTM D792
Water Absorption <= 0.040 %
@Time 86400 sec
<= 0.040 %
@Time 24.0 hour
ISO 62
Linear Mold Shrinkage 0.0020 - 0.0030 cm/cm0.0020 - 0.0030 in/in
Melt Flow 30 - 40 g/10 min
@Load 2.16 kg,
Temperature 230 °C
30 - 40 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 73 - 8073 - 801 sec, 2.00 mm; ISO 868
Tensile Strength at Break 30.0 - 50.0 MPa
@Thickness 2.00 mm
4350 - 7250 psi
@Thickness 0.0787 in
50 mm/min; ASTM D638
Tensile Strength, Yield 50.0 - 60.0 MPa
@Thickness 2.00 mm
7250 - 8700 psi
@Thickness 0.0787 in
50 mm/min; ASTM D638
Elongation at Break 20 - 300 %20 - 300 %50 mm/min; ASTM D638
Elongation at Yield 5.0 - 10 %5.0 - 10 %50 mm/min; ASTM D638
Tensile Modulus 1.80 - 2.60 GPa
@Thickness 2.00 mm
261 - 377 ksi
@Thickness 0.0787 in
1.0 mm/min; ASTM D638
Coefficient of Friction, Dynamic 0.15 - 0.350.15 - 0.35ASTM D1894
Coefficient of Friction, Static 0.20 - 0.400.20 - 0.40ASTM D1894
Taber Abrasion, mg/1000 Cycles 5.0 - 105.0 - 10CS-10 Wheel, 1000 g; ASTM D1044
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+14 ohm-cm>= 1.00e+14 ohm-cmASTM D257
Surface Resistance >= 1.00e+14 ohm>= 1.00e+14 ohmASTM D257
Dielectric Constant 7.0 - 10
@Frequency 1000 Hz
7.0 - 10
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 20.0 - 25.0 kV/mm
@Thickness 1.00 mm
508 - 635 kV/in
@Thickness 0.0394 in
ASTM D149
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 58.0 - 67.0 J/g25.0 - 28.8 BTU/lbASTM D3417
CTE, linear, Parallel to Flow 140 µm/m-°C
@Temperature 0.000 - 40.0 °C
77.8 µin/in-°F
@Temperature 32.0 - 104 °F
Specific Heat Capacity  1.20 J/g-°C
@Temperature 23.0 °C
0.287 BTU/lb-°F
@Temperature 73.4 °F
ASTM C351
 1.60 J/g-°C
@Temperature 100 °C
0.382 BTU/lb-°F
@Temperature 212 °F
ASTM C351
Thermal Conductivity 0.200 W/m-K
@Temperature 23.0 °C
1.39 BTU-in/hr-ft²-°F
@Temperature 73.4 °F
ASTM C177
Melting Point 170 - 175 °C338 - 347 °FDSC
Crystallization Temperature 134 - 144 °C273 - 291 °FPeak; ASTM D3418
 137 - 144 °C279 - 291 °FASTM D3418
Vicat Softening Point 135 - 145 °C275 - 293 °FRate A (50°C/h), Loading 2 (50 N)
Glass Transition Temp, Tg -40.0 °C-40.0 °FASTM E1356
Flammability, UL94 V-0
@Thickness 0.100 mm
V-0
@Thickness 0.00394 in
Oxygen Index 44 %
@Thickness 3.00 mm
44 %
@Thickness 0.118 in
ASTM D2863
 
Descriptive Properties
AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 Latin America
 North America
ColorWhite
FormPellets
Processing TechniqueExtrusion; Injection Molding

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Syensqo (Solvay Specialty Polymers) Solef® 32008 Polyvinylidene Fluoride (PVDF)
Arkema KYNAR® 370 Polyvinylidene Fluoride (PVDF) Homopolymer - Injection Molding
Syensqo (Solvay Specialty Polymers) Solef® 11008 PVDF Copolymer
3M Dyneon™ PVDF 6008/0001 Polyvinylidene Fluoride
3M Dyneon™ PVDF 32008/0009 Polyvinylidene Fluoride

PSOL8Y7286 / 177017

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.