MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hexcel® HexTow® AS2C Carbon Fiber  (discontinued **)
Categories: Carbon; Carbon Fiber/Carbon Fibre

Material Notes: HexTow™ AS2C carbon fiber is a continuous, high strength, high strain, PAN based fiber available in 3,000 (3K), 6,000 (6K), and 12,000 (12K) filament count tows. This fiber has been surface treated and can be sized to improve its interlaminar shear properties, handling characteristics, and structural properties. Suggested for use in weaving, prepregging, filament winding, pultrusion, and molding compounds.

Information provided by Hexcel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.80 g/cc0.0650 lb/in³Typical fiber property
Filler Content 62.0 %62.0 %Fiber Volume of Typical epoxy composite
Filament Diameter 6.9 µm6.9 µm
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 2140 MPa310000 psiTypical epoxy composite
 4470 MPa648000 psiTypical fiber property
Elongation at Break 1.9 %1.9 %Calculated from tow test data
Tensile Modulus 136 GPa19700 ksiTypical epoxy composite
 221 GPa32100 ksiTypical fiber property; Chord 6000-1000
Flexural Strength 1725 MPa250200 psiTypical epoxy composite
Flexural Modulus 128 GPa18600 ksiTypical epoxy composite
Shear Strength 124 MPa18000 psiTypical epoxy composite
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 94 %94 %Fiber
 
Descriptive Properties
Approximate Yield (m/g)1.2512K
 2.56K
 53K
Filament ShapeRound
Tow Cross-Sectional Area (mm2)0.113K
 0.226K
 0.4412K
TwistNone
Weight/Length (g/m)0.23K
 0.46K
 0.812K

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hexcel® HexTow® PV42/850 Carbon Fiber
Hexcel® HexTow® AS7 12K Standard Modulus Carbon Fiber
Hexcel® HexTow® AS4D Carbon Fiber - Epoxy Composite
Hexcel® HexTow® IM6 Carbon Fiber - Epoxy Composite
Hexcel® HexTow® AS4C 3K Standard Modulus Carbon Fiber (3000 Filaments)

EHECF0a / 101292

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.