UVI-6992 is a cationic photoinitiator containing a mixture of triarylsulfonium hexafluoroantimonate salts in propylene carbonate. UVI-6992 photoinitiator is used to UV-cure CYRACURE™ cycloaliphatic epoxide resins, vinyl ethers and other cationically curing materials. Information provided by Dow |