MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Alnico® 12 (Anisotropic, Cast) Hard Magnetic Alloy
Categories: Metal; Electronic/Magnetic Alloy; Nonferrous Metal

Material Notes: 33Fe-6Al-18Ni-35Co-8Ti

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.40 g/cc0.267 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 5858
Tensile Strength, Ultimate 275 MPa39900 psi
Modulus of Rupture 0.343 GPa49.7 ksiTransverse
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000620 ohm-cm0.0000620 ohm-cm
Magnetic Coercive Force, Hc 804 Oe804 Oe
Magnetic Remanence, Br 6000 Gauss6000 Gauss
Magnetic Maximum Energy Product, BH 1.76 MGOe1.76 MGOe
Curie Temperature 860 °C1580 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 11.0 µm/m-°C6.11 µin/in-°F
Maximum Service Temperature, Air 480 °C896 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 6.0 %6.0 %
Cobalt, Co 35 %35 %
Iron, Fe 33 %33 %
Nickel, Ni 18 %18 %
Titanium, Ti 8.0 %8.0 %
 
Descriptive Properties
Demagnetization Induction, Bd (Tesla)0.315
Intrinsic Magnetic Coercive Force, HCi (Oe)955

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Alnico® 9 (Anisotropic, Cast) Hard Magnetic Alloy
Alnico® 1 (Isotropic, Cast) Hard Magnetic Alloy
Alnico® 7 (Anisotropic, Cast) Hard Magnetic Alloy
Alnico® 8HC (Anisotropic, Cast) Hard Magnetic Alloy
Chromindur® II Hard Magnetic Alloy

MM907 / 100414

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.