MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Atom Adhesives AA-DUCT 906 Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: AA-DUCT 906 is based on a silver coated ceramic that results in lower material costs without adversely sacrificing the properties obtained with a pure silver formulation. This concept opens the door to a wide range of applications previously prohibited by the much higher cost of conventional silver conductive. AA-DUCT 906 cures at room temperature or can be accelerated with mild heat to form a tenacious bond between similar and dissimilar substrates such as aluminum, copper, magnesium, steel, bronze nickel, ceramic, glass, phenolic, and G-10 epoxy glass boards. AA-DUCT 906, because of its excellent continuity, has been used extensively in such diversified applications as, microwave EMI and RFI shielding, in the assembly or repair of printed circuit boards, wave guides, electronic modules, flat cable, high frequency shields, connections, and circuitry and as a cold solder. This unique formulation offers ease in handling due to its creamy consistency and versatile application by hand, automatic dispenser, silk-screening, transfer or stamping techniques

Appearance: Silver

Cure Type: Heat cure or Room Temperature

Benefits:

  • High strength
  • Perfect bond
  • EMI & RFI shielding
  • Cold Solder
Mix Ratio by weight: 100:5/Resin:Hardener

Substrates: Excellent choice aluminum, copper, magnesium, steel, bronze, nickel, kovar, ceramic, glass, phenolic and G-10 epoxy glass boards.

Typical Application: microwave EMI and RFI shielding, in the assembly or repair of printed circuit boards, wave guides, electronic modules, flat cable, high frequency shields, connections, and circuitry and as a cold solder

Information provided by Atom Adhesives

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.60 g/cc2.60 g/cccured
Linear Mold Shrinkage 0.0040 cm/cm0.0040 in/incured
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8181cured
Tensile Strength 61.4 MPa8900 psicured
Compressive Strength 94.5 MPa13700 psicured
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 0.0015 ohm-cm<= 0.0015 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 19.0 µm/m-°C10.6 µin/in-°F
Thermal Conductivity 13.0 W/m-K90.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 165 °C329 °F
Heat Distortion Temperature 165 °C329 °F
Minimum Service Temperature, Air -50.0 °C-58.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  15.0 min
@Temperature 100 °C
0.250 hour
@Temperature 212 °F
 30.0 min
@Temperature 60.0 °C
0.500 hour
@Temperature 140 °F
 1440 min
@Temperature 25.0 °C
24.0 hour
@Temperature 77.0 °F
Shelf Life 12.0 Month12.0 Monthuncured
 
Descriptive Properties
ViscosityPasteuncured

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trelleborg Emerson & Cuming Eccobond® 57C Two-Component Silver Filled Electrically Conductive Epoxy Adhesive
Toho Tenax Besfight® G40-800 6K IMA-5C EP03 Continuous Filament Carbon Fiber
Toho Tenax Besfight® G30-500 6K HTA-7C EP01 Continuous Filament Carbon Fiber
Solvay Thornel® T-300 6K Carbon Fiber, Polyacrylonitrile (PAN) Precursor
SGL Carbon Group PANOX® SA T320 EEA High performance oxidized textile fiber, Continuous Tow with 320k filaments

PATOM035 / 172350

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.