MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Permabond 738 Cyanoacrylate, toughened
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: PERMABOND 738 is a toughened cyanoacrylate with improved impact and peel strength when compared to a conventional cyanoacrylate. It bonds rapidly at room temperature and its viscosity is stable over the shelf life of the product. This provides consistent performance. The product adheres to a variety of surfaces including steel, aluminum, galvanized steel, plastics and elastomers.

Features and Benefits:

  • Provides better impact and peel strength
  • Bonds in 20-30 seconds to most surfaces
  • Color is suitable for matching dark surfaces
  • Material is capable of curing through gaps as large as 0.020 inches

Soluble In Nitroethane, Methyl Ethyl Ketone, Acetone.

Information provided by Permabond.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 g/cc1.10 g/ccUncured
Solids Content 100 %100 %
Viscosity 5000 cP
@Temperature 25.0 °C
5000 cP
@Temperature 77.0 °F
Uncured
Storage Temperature 2.00 - 7.00 °C35.6 - 44.6 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8585
Adhesive Bond Strength 21.0 MPa3050 psiGrit-blasted Steel, Shear
Impact 16.816.8kJ/m2 Adhesive Impact Strength; ASTM D950
Peel Strength 2.28 kN/m13.0 pliASTM D903
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 9.84 kV/mm250 kV/in
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 82.0 °C180 °F
Minimum Service Temperature, Air -60.0 °C-76.0 °F
Flash Point 83.0 °C181 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 0.0833 - 0.167 min0.00139 - 0.00278 hourPhenolic, set time, cured
 0.167 min0.00278 hourSteel, set time
 0.167 min0.00278 hourBuna N Rubber, set time
 0.167 min0.00278 hourPhenolic, set time
 0.167 - 0.250 min0.00278 - 0.00417 hourBuna Rubber, set time, cured
 0.417 - 0.500 min0.00694 - 0.00833 hourSteel, set time, cured
 0.500 - 0.583 min0.00833 - 0.00972 hourAluminum, set time, cured
 1440 min
@Temperature 25.0 °C
24.0 hour
@Temperature 77.0 °F
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
AppearanceBlackUncured
Maximum Gap Fill (mm)0.51

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
International Mold Steel NAK80 Precipitation Hardened Mold Steel
IN-738 Cast Nickel Superalloy
Special Metals INCONEL® alloy 783 Ni-Co-Fe Alloy
Nitriflex N-6011 NBR - Nitrile Rubber
Nimocast 738 Superalloy

PPERMA866 / 162758

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.