Market Segment: Compounding Suggested Uses Include Compounding and Thermoforming Information provided by Sunoco Chemicals. Available in Canada. Braskem acquired Sunoco Chemicals polypropylene product line in 2010. |
Extra High Izod Impact, Very High Flexural Modulus, Good Low Temperature Drop Impact |