MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Pyrotek Pyrocast AL3 Abrasion & Alkali Resistant Refractory Castable
Categories: Ceramic; Oxide; Aluminum Oxide; Silicon Oxide

Material Notes: Pyrocast AL3 is suited for use in aluminum melting equipment and metal transfer areas where sever wear or alkali attack are a factor. Pyrocast AL3 is a high-purity mullite based refractory with low iron content.

Applications

  • Aluminum melting equipment
  • Aluminum holding equipment
  • Transfer troughs
  • Ladle linings

Advantages

  • Outstanding hot strength
  • Excellent abrasion resistance
  • Resists alkali attack
  • Resists molten aluminum attack

Information provided by Pyrotek.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.675 g/cc0.09664 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture 0.0386 GPa
@Temperature 816 °C
5.60 ksi
@Temperature 1500 °F
Hot
 0.0200 GPa
@Treatment Temp. 110 °C
2.90 ksi
@Treatment Temp. 230 °F
fired and cooled
 0.0280 GPa
@Treatment Temp. 954 °C
4.06 ksi
@Treatment Temp. 1750 °F
fired and cooled
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  1.56 W/m-K
@Temperature 260 °C
10.8 BTU-in/hr-ft²-°F
@Temperature 500 °F
 1.59 W/m-K
@Temperature 538 °C
11.0 BTU-in/hr-ft²-°F
@Temperature 1000 °F
 1.69 W/m-K
@Temperature 816 °C
11.7 BTU-in/hr-ft²-°F
@Temperature 1500 °F
 1.83 W/m-K
@Temperature 1093 °C
12.7 BTU-in/hr-ft²-°F
@Temperature 1999 °F
Maximum Service Temperature, Air 1704 °C3099 °F
Shrinkage 0.20 %
@Temperature 954 °C
0.20 %
@Temperature 1750 °F
Linear

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Pyrotek Pyrocast AL2 Abrasion-Resistant Refractory Castable
Pyrotek Pyrocast AR Castable Refractory
Pyrotek Pyrocast AR PLUS Castable Refractory
Pyrotek Pyrocast ALF3 Low Cement Refractory Castable
Pyrotek Pyrocast PCR Abrasion-Resistant Refractory Castable

CPYRO172 / 1889

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.