MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Silikony Polskie Gumosil AD-1 A/B Silicone Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone; Silicone Rubber

Material Notes: Flexible with high resistance to tension

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 g/cc1.10 g/ccBefore Curing
Viscosity 20000 cP20000 cPBefore Curing
Linear Mold Shrinkage 0.0010 - 0.0020 cm/cm0.0010 - 0.0020 in/inAfter Curing
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 2525After Curing
Tensile Strength at Break 8.00 MPa1160 psiAfter Curing
Elongation at Break 650 %650 %After Curing
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 180 °C356 °F
 
Processing PropertiesMetricEnglishComments
Cure Time <= 960 min<= 16.0 hourCuring
Pot Life 60 min60 minCuring
 
Descriptive Properties
ColorPink, translucent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Polychloroprene Rubber (CR)
Silikony Polskie Gumosil B Silicone Rubber
Overview of materials for Silicone Rubber
Momentive Performance Materials TUFEL™ II 94305 Low Volatile Extrusion Heat Cured Rubber
Momentive Performance Materials TUFEL™ II 94205 Low Volatile Extrusion Heat Cured Rubber

PPOLSI010 / 84310

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.